This site will look much better in a browser that supports web standards, but it is accessible to any browser or Internet device.

Instron Structural Testing

The Test Solutions Provider!

Elastomeric Testing Systems

IST elastomeric testing systems are available in different configurations to suit your testing requirements. These systems are designed for application testing of such things as visco-elastic properties of rubber-metal components and hydromounts such as axle mounts or motor bearings. IST has a comprehensive range of single and multiple axial rigs which operate at various test frequencies and loads. Below we showcase a small range of realized standard systems for elastomeric tests. All other configurations are only on request.

Medium high frequency elastomer testing system for single-axis testingSelect image to enlarge MHF 25I Medium High Frequency (MHF) Testing Machines

Medium high frequency testing machines for single-axis testing

  • Test frequencies: up to 400 Hz depending on actuator used
  • Nominal load: 10/25/50 kN
  • Displacement: ± 10/25/50 mm

Medium high frequency elastomer testing system for two-axis testingSelect image to enlarge MHF 25I / 5I Medium High Frequency (MHF) Testing Machines

Medium high frequency testing machines for bi-axial testing

  • Test frequencies: up to 200 / 400 Hz
  • Nominal load: 25 kN / 5 kN
  • Displacement: ± 25 mm

Very high frequency (MHF) testing machines for single-axis testingSelect image to enlarge VHF 7D Very High Frequency (VHF) Testing Systems

Very high frequency testing system for single-axis testing

  • Test frequencies: up to 1000 Hz
  • Nominal load: 7 kN
  • Displacement: ± 10 mm

Additional torsion test setup for VHF 7DSelect image to enlarge VT 1.000 Additional Torsion Test Setup for VHF 7D

  • Torsional vibration isolator test
  • Test frequencies: up to 650 Hz
  • Nominal load: 1 kNm
  • Angle: ± 4°
  • Bearing mounted in a 2-column VHF machine

Two axial elastomer testing system with hydrostatic side load table VHF 10D / 3I Very High Frequency (VHF) Testing Systems

Very high frequency testing system for bi-axial testing

  • Bi-axial VHF testing systems for high frequency testing of engine mounts under lateral side load
  • Variable side load capacity dependent on maximum test frequency
  • Hydrostatic sliptable with multi-axial load measuring platform (Kistler)
  • Test frequencies: up to 400 Hz
  • Nominal load: 10 kN / 3 kN
  • Displacement: ± 10 mm / ± 25 mm
  • Lateral side load via hydrostatic sliptable (Limited Frequency Response)
  • Crosshead control via separate control channel
  • Climatic chamber temperature control

Multi-axial elastomeric testing systemSelect image to enlarge MAETS 3L Multi-Axial Elastomeric Testing System

  • Lateral 3-axis load configuration
  • Maximal frequency: 80 / 100 Hz
  • Linear load: 25 kN
  • Displacement: ± 25 mm

Multi-axial elastomeric testing systemSelect image to enlarge MAETS 3L 1R Multi-Axial Elastomeric Testing System

Designed for durability test of passenger car axle and engine mounts.

  • Lateral 3-axis, torsion 1-axis load
  • Maximal frequency: 80 Hz
  • Linear load: 25 kN
  • Displacement: ± 25 mm
  • Torque: Max 1 kNm
  • Angle: ± 30°

Low Frequency Torsional Test SystemsSelect image to enlarge LFT Low Frequency Torsional Test Systems

  • Test frequencies: up to 400 Hz depending on rotary actuator used
  • Nominal load: 1 - 64 kNm
  • Angle: ± 50°

High frequency torsional testing systemSelect image to enlarge HFT High Frequency Torsional Test Systems

  • Test frequencies: up to 700 Hz
  • Nominal load: 2 kNm
  • Angle: ± 5°

Quality check systems for production lineSelect image to enlarge Quality Assurance Systems for Production Line Applications

  • Rotary damper checking
  • Automatic checking systems for engine mounts with statistical evaluation

 

Related Links

Application example - Durability Testing
Application example - Squeak and Rattle Testing

LabSite™ and Labtronic™ are trademarks of Instron and LabSite® and Labtronic® are registered trademarks of Instron in Germany.