Common Standards for Compression Tests
Plastics
Metals
- ASTM E9
- ASTM E209-00(2005)
- ISO 4506
- BS EN ISO 8492
Concrete and Cement
- ASTM C109
- BS EN 12390-3
- EN 196-1
- ISO 679
Spring
Wood
- DIN 52185
- DIN 52192
- ISO 3132
Instron manufactures a complete range of compression testers for determining the compressive strength of countless materials and meeting the needs of the transportation, construction, and consumer products industries. Compression testing systems utilize varying technologies, such as electromechanical, static hydraulic for high-capacity compression tests, and dynamic with the capability of performing both static and dynamic tests.
Electromechanical compression test systems are crosshead-driven systems characterized by the use of pre-loaded ball screws, guidance columns and digital closed-loop position control. Frame configurations include a single column tester; table or dual column model; and floor models.
High-capacity SATEC™ series systems perform compression tests using static hydraulic technology. This family of universal testers includes some of the most rugged and durable machines ever made. These frames are powered by a hydraulic pumping system that moves a piston assembly to provide the forces necessary for testing.
Dynamic systems are capable of performing both static compression and fatigue tests. The state-of-the-art ElectroPuls™, a new family of lower force electrodynamic test instruments, are all-electric and require no air, hydraulics, water or special utilities.
|
Electromechanical
Compression testers
|
SATEC Series
High-capacity compression testers
|
Dynamic
Static and fatigue testers
|
|
|
|
3340, 5540, 5840 Single Column Models
- 500 N (112 lbf) to 5 kN 1,100 lbf)
3360, 5560, 5860 Table Models
- 5 kN (1,100 lbf) to 50 kN 11,250 lbf)
3380, 5580, 5880 Floor Models
- 50 kN (11,250 lbf) to 600 kN (135,000 lbf)
|
KN Models
- 300 kN (67,500 lbf ) to 3500 kN (785,000 lbf)
LX/DX Models
- 150 kN (33,750 lbf ) to 600 kN (135,000 lbf)
HVL Models
- 300 kN (67,500 lbf ) to 3000 kN (670,000 lbf)
HDX Model
|
ElectroPuls
- 1 kN (225 lbf ) to 3 kN (675 lbf)
8870 Table Models
- 5 kN (1,125 lbf) to 25 kN (5,620 lbf) with Torsion
8801, 8802 Floor Models
- 10 kN (2,250 lbf) to 250 kN (56.250 lbf)
8803, 8804, 8805, 8806 Floor Models
- 250 kN (56,250 lbf) to 2500 kN (562,500 lbf)
|
Specialized Compression Testers
|
Concrete Testing: The SATEC RD Series Compression Tester is ideally suited for advanced concrete compression testing where frame stiffness is critical and is available in capacities ranging from 2,000 kN (400,000 lbf) – 5,000 kN (1,100,000 lbf). Common materials tested in compression include concrete cylinders, cubes, masonry blocks and bricks.
|
|
Soils Testing: The DX compression-only testing system can be equipped with automatic exudation detection for soils. Audio prompting and an extended tabletop help make stabilometer testing more efficient and user-friendly for both soils and asphalt testing. Additional features include an upper spherical compression plate with lockout ring eliminating the need for shims.
|
|
Spring Testers: The SF Series spring testers incorporate all the features required to make spring testing easy, accurate, and efficient at a very competitive price. Designed for load testing all types of coil springs, disc springs, wave springs, leaf springs and spring-type components, this cost-effective series is capable of testing springs from 0.5 kN to 100 kN (112 lbf to 22,500 lbf)..
|
Common Accessories and Software for performing Compression Tests
|