The physical condition of your tup insert can adversely affect your impact test
data?
Tup inserts that are worn, flattened, scratched, or chipped can actually change
the characteristics of your test. These changes may show up in your data in the
form of higher loads or longer times to failure. Be sure to inspect your tup insert
periodically for signs of wear and tear.
View our Dynatup Impact Testing Accessories
for further information
|