Charpy and Izod Pendulum Impact Tester for Metals — SI Series

Charpy and Izod Pendulum Impact Tester for Metals— SI Series

Ideal for Izod and Charpy metals impact testing, the SI Series is well known for its rugged design, high accuracy and low operating costs.

Features
  • Available in five floor models with capacities ranging from 25-300 ft-lb
  • Per ASTM E-23 standard
  • Select models capable of N.I.S.T. Charpy tests
  • Data acquisition software available
Range of Models
SI-1A*
  • Low capacity 25 ft-lbs
  • High capacity 60 ft-lbs
  • Dial Increments .25 ft-lbs
  • Tests Charpy & Izod
SI-1B*
  • Low capacity 25 or 50 ft-lbs
  • High capacity 60 or 120 ft-lbs
  • Dial Increments .25 or .50 ft-lbs
  • Tests Charpy & Izod
SI-1C3
  • Low capacity 170 Joules (125 ft-lbs)
  • High capacity 407 Joules (300 ft-lbs)
  • Dial Increments 2.0 Joules (1 ft-lb)
  • Tests Charpy & Izod
SI-1D3*
  • Low capacity 25, 50, or 120 ft-lbs
  • High capacity 60, 120, or 300 ft-lbs
  • Dial Increments .25, .50, or 1 ft-lbs
  • Tests Charpy & Izod
SI-1K3
  • Low capacity 170 Joules (125 ft-lbs)
  • High capacity 407 Joules (300 ft-lbs)
  • Dial Increments 2.0 Joules (1.0 ft-lb)
  • Tests Charpy
 
System Options
  • Suited for use with instrumented tups and Dynatup Impulse data acquisition and analysis system
  • *Models also available with metric dial readings