R.R. Moore Rotating Beam Fatigue Testing Machines are recognized as the industry standard for rotating beam fatigue testing and rotating each specimen through an average of 9,999 complete stress cycles per minute. Bending stress is applied to the specimen by means of dead weights. A digital indicator provides the number of completed cycles with automatic shut-off upon specimen failure and provides an indication of the operating speed (rotations per minute or RPM.)
Features
- Capacity of 25 kg-cm to 230 kg-cm (20 in-lb to 200 in-lb) in 0.254 kg-cm (0.2 in-lb) increments
- Variable rotation speeds from 1,000 to 9,999 RPM
- Easy to read digital rpm speed indicator and cycle counter
- Automatic shut-off switch
- Drawbars for machined taper-end specimens
Options and accessories
- Drawbars and collets for straight shank specimens
- High temperature furnace and temperature control system for elevated temperature testing
|