Instron® Bluehill® Fracture Standards Library

SYNOPSISBluehill Fracture Standards Library is a Microsoft Windows PC compatible software package, developed by Instron - Division of ITW Limited, that provides a library of analysis functionality used by the Instron Bluehill Fracture software.
Brittle KIc
|
Specimens
supported |
|
ASTM E399-20ª | CT Load Line | |
CT Front Face | ||
SENB | ||
Disk Front Face | ||
Disk Load Line | ||
Arc Tension | ||
Arc Bend | ||
ISO 12135:2021 | CT Load Line | |
CT Front Face | ||
SENB | ||
ASTM B645 (ASTM E399-20a) | CT Load Line | |
BS 7448-1:1991 | CT Load Line | |
CT Front Face | ||
SENB |
Brittle J/CTOD
|
Specimens
supported |
|
BS 7448-1:1991 | CT Load Line | |
CT Front Face | ||
SENB |
Ductile JIc/CTODIc
|
Specimens
supported |
|
ASTM E1820-20b | CT Load Line | |
SENB |
||
Disk Load Line |
Ductile DCPD (JIc/CTODIc)
|
Specimens
supported |
|
ASTM E1820-20b | CT Load Line | |
SENB | ||
Disk Load Line |
Crack growth
|
Specimens
supported |
|
Crack growth - compliance or DCPD (ASTM E647 & ISO 12108 – control and recording only - excludes analysis) | CT Load Line | |
CT Front Face | ||
SENB | ||
Disk Front Face | ||
Disk Load Line | ||
Arc Tension | ||
MT Uniform stress | ||
MT Uniform displacement | ||
MT Pin loaded |
RELEASE NOTES
Version 2.0 Build 22018.01 (18/January/2022)
- Support added for:
- J Integral calculation to BS7448-1:1991
- J Integral calculation to E1820-20b (Annex 18 - DCPD Method)
- ISO 12135:2021
- KIC ISO12135:2021
- Requires Bluehill Fracture V2.0 or later
Version 1.3. (20/May/2021)
- Support added for:
- E399-20a
- E1820-20b
- BS-7448-1:1991 - CTOD Calculation
- Requires Bluehill Fracture V1.3 or later
Version 1.2. Build 20167 (23/Jun/2020)
- Support added for:
- E399-20
- E1820-20ε1
- Requires Bluehill Fracture V1.2 or later
Version 1.2. Build 20063 (10/Mar/2020)
- Support added for:
- Crack Growth tests
- Disk CT Load Line, Disk CT Front Face, and Arc Tension specimens
- ASTM E1820-20 analysis of JIC and CTOD only
- Requires Bluehill Fracture V1.2 or later
Version 1.1 (07/Nov/2019)
- Support added for:
- ASTM E399-19 analysis of KIC only
- ASTM B645-10 analysis of KIC only
- ASTM E1820-18a analysis of JIC and CTOD only
- Requires Bluehill Fracture V1.1 or later
Version 1.0 (04/Feb/2019)
- Initial release with support for:
- ASTM E399-2017 analysis of KIC only
- ASTM E399-2012 analysis of KIC only
- BS 7448-1:1991 analysis of KIC only
- ISO 12135:2016 analysis of KIC only
- ISO 12135:2002 analysis of KIC only
- Requires Bluehill Fracture V1.0 or later