0.357 Inch Shoulder-End Specimen Inserts, 200 kN
W-5158-B | 0.357 inch shoulder-end specimen inserts, One Set
Static Tensile Capacity: 200kN
Instron standard specimen: 231249-2, Ref. ASTM A370, Figure 4
Requirement: W-5158 300kN Insert Holder
Capacity | 200 kN (45,000 lbf) |
---|---|
Static or Fatigue Rated | Static |
Temperature Rating | 0-38°C (32-100°F) |
Split Insert Tensile Grips W-5158 and W-5159
Instron® Split Insert Tensile Grips are designed for safe, high-volume production testing of shoulder-end or button-head machined specimens. Engineered with an operator focus, the split insert style tensile grips are easy to install, offer quick change inserts for standard specimen sizes, and promote efficient testing of a wide range of metals and alloys.