Damping is the dissipation of energy in motion of any type.
Viscosity of fluids is a damping effect, and is highly dependent on deformation rate.
Damping is also related to procedures to reduce vibrations during impact tests (typically instrumented tests, to improve the force signal reading), for example putting a soft layer between two metal striking parts.