Ductile Failure (Impact)
Material failure mode that is characterized by a significant yielding and plastic deformation along with cracking. The load-time curve for an instrumented impact shows a zero-slope area around the maximum and extends in time beyond the point of maximum load, with the specimen still absorbing energy.
In drop tower tests, the tup (falling dart) leaves a hole or rupture through the full thickness of the specimen rather than cracking outwardly form the point of failure. The impact area shows elongated and thinned parts.
Serie 3400 – Erschwingliche Testlösungen
Instron Serie 3400 Universal-Testsysteme für Zug, Kompression, Biegung und andere Materialeigenschaften-Tests.
Broschüre Serie 6800 Premier Testing Systems
Universal-Testsysteme der Instron Serie 6800 bieten unvergleichliche Genauigkeit und Zuverlässigkeit. Die 6800 Serie basiert auf einer zum Patent angemeldeten Operator-Protect-Systemarchitektur mit einem brandneuen Smart-Close Air Kit und Collision-Mitigation-Funktionen, wodurch Materialtests einfacher, intelligenter und sicherer sind als je zuvor.
Broschüre Bluehill Universal
Bluehill Universal wurde von Grund auf für haptische Interaktion und eine intuitive Benutzererfahrung ausgelegt. Entdecken Sie einfacheres und schnelleres Prüfen mit Funktionen wie vorgeladene Prüfmethoden, QuickTest in Sekunden, verbessertem Datenexport und Instron Connect, einer neuen Funktion, die eine direkte Verbindung zum Service bereitstellt. Benutzer früherer Versionen von Software wie Bluehill 2 und Bluehill 3 können leicht auf die neueste Version von Bluehill aufrüsten.