Total Absorbed Energy (Impact)

The amount of energy that the specimen absorbed during the entire impact test – from start to end. This value may be the same as energy to maximum load when the specimen abruptly fails at the maximum load point. The value is calculated from the time the load begins to rise until the first occurrence of 0 load after the maximum point. This value can be used as an indicator to a materials ductility or toughness – the higher the value the stronger the material. However, are needs to be taken to ensure that when the data collection ends, the load has fallen below the 0 threshold. If it hasn’t, this value is no longer a valid number to be used.

Related Content

Serie 3400 – Erschwingliche Testlösungen

Instron Serie 3400 Universal-Testsysteme für Zug, Kompression, Biegung und andere Materialeigenschaften-Tests.

Broschüre Serie 6800 Premier Testing Systems

Universal-Testsysteme der Instron Serie 6800 bieten unvergleichliche Genauigkeit und Zuverlässigkeit. Die 6800 Serie basiert auf einer zum Patent angemeldeten Operator-Protect-Systemarchitektur mit einem brandneuen Smart-Close Air Kit und Collision-Mitigation-Funktionen, wodurch Materialtests einfacher, intelligenter und sicherer sind als je zuvor.

Broschüre Bluehill Universal

Bluehill Universal wurde von Grund auf für haptische Interaktion und eine intuitive Benutzererfahrung ausgelegt. Entdecken Sie einfacheres und schnelleres Prüfen mit Funktionen wie vorgeladene Prüfmethoden, QuickTest in Sekunden, verbessertem Datenexport und Instron Connect, einer neuen Funktion, die eine direkte Verbindung zum Service bereitstellt. Benutzer früherer Versionen von Software wie Bluehill 2 und Bluehill 3 können leicht auf die neueste Version von Bluehill aufrüsten.

Kontakt

Kontakt

Weitere Informationen über unsere Branchen- und Testlösungen erhalten Sie, wenn Sie uns kontaktieren. Unsere Kundendienst- und Serviceteams stehen bereit, Ihnen behilflich zu sein.