Bestimmung der internen Bindungsfestigkeit an Faserplatten und Holzklebstoffen nach ASTM D1037

ASTM D1037 solutions

ASTM D1037, the Standard Test Method for Evaluating Properties of Wood-Base Fiber and Particle Panel Materials, outlines multiple testing procedures to characterize the mechanical properties of fiberboard. The internal bond test procedure is outlined in section 11 of the ASTM D1037 standard, though other sections also evaluate fastener holding, flexure properties, and compression properties in ambient or simulated environmental conditions.

Wood fiberboard is an engineered material made by using an adhesive to glue wood chips or wood particles together under high pressure, and the internal bond test of ASTM D1037 ensures that the cohesion strength of the engineered panel is sufficient for a given application. The internal bond test measures the tensile strength of the material when applying a force perpendicular to the face. This testing is especially important considering that these materials are used in construction applications and many of them are formed through the adhesion of multiple layers of material.

Materials Testing System

Most ASTM D1037 force requirements are suitable for a dual column universal testing system such as those found in Instron's 6800 and 3400 Series. Required fixtures include Instron's 2820-061 internal bond test fixture and 2820-062 steel specimen blocks, which were designed in compliance with the requirements of this standard. 




ASTM D1037
1) 6800 Series Universal Testing System
2) Bluehill Universal Software
3) 2580 Series Load Cell
4) 2820-061 Internal Bond Fixture for Wood and Fiberboard

 

ASTM D1037 test setup
ASTM D1037 Test Fixtures 

The principle of ASTM D1037 internal bond testing involves bonding specimen blocks to the top and bottom surfaces of the test specimen with a suitable adhesive. The loading block bond must be stronger than the expected failure force of the specimen. The upper loading fixture should be self-aligning, and the specimen blocks should be 2-inch square by 1-inch in thickness and made from steel or aluminum alloy. Instron’s 2820-061 and 2820-062 fixtures have been designed in compliance with these requirements.

Related Content

Broschüre Serie 6800 Premier Testing Systems

Universal-Testsysteme der Instron Serie 6800 bieten unvergleichliche Genauigkeit und Zuverlässigkeit. Die 6800 Serie basiert auf einer zum Patent angemeldeten Operator-Protect-Systemarchitektur mit einem brandneuen Smart-Close Air Kit und Collision-Mitigation-Funktionen, wodurch Materialtests einfacher, intelligenter und sicherer sind als je zuvor.

Serie 3400 – Erschwingliche Testlösungen

Instron Serie 3400 Universal-Testsysteme für Zug, Kompression, Biegung und andere Materialeigenschaften-Tests.

Broschüre Bluehill Universal

Bluehill Universal wurde von Grund auf für haptische Interaktion und eine intuitive Benutzererfahrung ausgelegt. Entdecken Sie einfacheres und schnelleres Prüfen mit Funktionen wie vorgeladene Prüfmethoden, QuickTest in Sekunden, verbessertem Datenexport und Instron Connect, einer neuen Funktion, die eine direkte Verbindung zum Service bereitstellt. Benutzer früherer Versionen von Software wie Bluehill 2 und Bluehill 3 können leicht auf die neueste Version von Bluehill aufrüsten.

2820-061 Interne Bindungsvorrichtung für Holz

Die 2820-061 interne Bindungsvorrichtung ist für die Prüfung der Festigkeitseigenschaften von Holz- oder Klebstoffbindungen in Holz durch Zugbelastung ausgelegt.