ISO 527-3 is an international standard used to determine the tensile properties of plastic film or sheeting. Plastic films are used extensively in the packaging industry and as components of more complex products, such as electric vehicle batteries. Material properties reported for this standard are tensile strength, yield point, and strain.

Film or sheeting is defined to be a plastic test specimen with a thickness less than 1 mm. Plastics with a thickness greater than 1 mm should be tested per ISO 527-2. The equivalent ASTM standard to ISO 527-3 is ASTM D882.




ASTM D3330 Test Setup
6800 Series Universal Testing System
 Bluehill Universal Software
 2580 Series Load Cell
 Pneumatic Side-Action Grips

 

ISO 527-3 test setup
Gripping Solutions 

Due to the flexible, delicate nature of thin film specimens, specimen gripping can be a challenge. Pneumatic side action grips are an ideal solution because they provide an adjustable inlet air pressure to ensure that specimens can be clamped sufficiently throughout the test. When using pneumatic grips with the Smart-Close Air Kit, operators can define the inlet clamping pressure in the Bluehill Universal test method, replacing the need to manually change the pressure at the air supply’s regulator. The Smart-Close Air Kit not only promotes a safer use of pneumatic grips, but it can make testing more efficient and repeatable.


For those looking for a non-pneumatic solution for ISO 527-3 testing, Instron recommends self-tightening roller grips. Manually-tightened screw grips are not recommended for thin film testing, because the variability they add to the clamping pressure can negatively impact the repeatability of results and cause a higher frequency of improper gripping (jaw breaks or slippage). 

2712-041
1 kN Model | 2712-041
2613-007
1 kN Model | 2713-007
Strain Measurement

While ISO 527-3 does not require extensometry, the use of an extensometer always results in the most accurate strain measurement. Non-contacting video extensometry is the best solution for thin film testing, as typical clip-on extensometers weigh down the specimen causing premature failure. Instron's Advanced Video Extensometer (AVE2) can measure strain as accurately as a clip-on extensometer without physically contacting the specimen.

Results and Throughput

Instron's Bluehill® Universal testing software makes it easy to report calculations in compliance with the standard. Customers who choose the Plastics method suite will receive a pre-configured test method for ISO 527-3 testing, complete with specific test parameters and calculations to help ensure compliance.

For labs with high-volume testing needs, several modifications to the tensile machine setup can be made to speed up the testing process and increase throughput, up to and including fully automated test systems. Fully automated systems such as Instron's AT3 are designed to incorporate specimen measurement, specimen loading, testing, and removal, and are able to run for hours without operator interaction. These systems help to reduce variability due to human error and can be left running after a shift ends to continue getting results when operators go home.


Related Content

6800 Serie – Broschüre für Premium-Testsysteme

Universal-Testsysteme der Instron Serie 6800 bieten unvergleichliche Genauigkeit und Zuverlässigkeit. Die 6800 Serie basiert auf einer zum Patent angemeldeten Operator-Protect-Systemarchitektur mit einem brandneuen Smart-Close Air Kit und Collision-Mitigation-Funktionen, wodurch Materialtests einfacher, intelligenter und sicherer sind als je zuvor.

Broschüre Bluehill Universal

Bluehill Universal wurde von Grund auf für haptische Interaktion und eine intuitive Benutzererfahrung ausgelegt. Entdecken Sie einfacheres und schnelleres Prüfen mit Funktionen wie vorgeladene Prüfmethoden, QuickTest in Sekunden, verbessertem Datenexport und Instron Connect, einer neuen Funktion, die eine direkte Verbindung zum Service bereitstellt. Benutzer früherer Versionen von Software wie Bluehill 2 und Bluehill 3 können leicht auf die neueste Version von Bluehill aufrüsten.

Serie 3400 – Erschwingliche Testlösungen

Instron 3400 Serie Universal-Testsysteme für Zug, Kompression, Biegung und andere Materialeigenschaften-Tests.

2712-04X Serie – Seitlich wirkende, pneumatische Spannzeuge

Seitlich wirkende, pneumatische Spannzeuge sind eine vielseitige Lösung zum Einspannen vieler Materialien. Bewertete Kapazitäten zwischen 1 und 10 kN.

2713-007 Serie Selbstspannendes Spannzeug mit Rolle

Die selbstspannenden Spannzeuge sind in erster Linie für die Präzisionsprüfung von Elastomeren und anderen flexiblen Materialien konzipiert, die eine große Reduzierung der Querschnittsfläche unter Last aufweisen.

Berührungsloses Video-Extensometer AVE 2

Das erweiterte Video-Extensometer (AVE 2) setzt patentierte Messtechnologie in dem schnellsten und genauesten berührungslosen Gerät zur Dehnungsmessung auf dem Markt ein.