a. The ability of a material to withstand shock loading.
b. The work done in fracturing under shock loading. a specific test specimen in a specified manner.
A measure of the resiliency or toughness of a solid. The maximum force or energy of a blow (given by a fixed procedure) which can be withstood without fracture, as opposed to fracture strength under a steady applied force.