E-Series Deflectometer
W-E401-H | E-Series Deflectometer
Displacement Strain Deflectometer. Often used for measuring deflection in 3 or 4 point bending tests, on compression tests and for a variety of general test deflection measurements. Includes magnetic base for easy mounting.
Specifications:
- Travel: 25 mm
- Standard Temp. Range: -40°F to 210°F (-40°C to 100°C)
Instrument supplied with Instron standard 25 pin connector.
Compatible Frame Models | All |
---|---|
Static or Fatigue Rated | Static |