2530 Series load cells with capacities of 5 N to 100 N are for use with 6800, 3400, 5900, and 3300 Series testing systems. 2530 Series Load cells with capacities of 500 N to 300 kN are for use with 3400 and 3300 testing systems. The design, manufacture, and performance verification is conducted with materials testing applications in mind. Automatic transducer recognition and electrical calibration makes them easy to use. The load cells incorporate overload protection and can withstand loads up to 150% of their force capacity without damage and 300% without mechanical failure. The load cells allow the user to zero out the tare weight of a grip or fixture that weighs up to 10% or 40% of the force capacity, depending on the model, while still maintaining the full specified accuracy.
All Instron load cells are individually temperature-compensated and tested for accuracy and repeatability on calibration apparatus that is traceable to international standards, with a measurement uncertainty that does not exceed one-third of the permissible error of the load cell.
Application Range- Suitable for a range of test types, including tension, compression, cyclic, and reverse stress
- Accurate measurements down to 1/500th of load cell capacity means fewer load cells and fewer load cell changes
- Automatic recognition with electronic serial number and electrical calibration allows for simple, error-free operation
- Tare weight 10% or 40% of force capacity, depending on model – can be used with a wide range of grips and fixtures
- Complies with all international force measurement standards, including ASTM E4, ISO 7500-1 class 0.5, and JIS B7721, B7733
Item Name | Capacity | Mechanical Fitting | Cat # |
---|---|---|---|
5 N Static Load Cell | .005 kN 1.12 lbf | 2.5mm Clevis Pin with 6mm Adapter (Type OOf & Of) | 2530-5N |
10 N Static Load Cell | .01 kN 2.25 lbf | 2.5 mm Clevis Pin with 6 mm Adapter (Type OOf & Of) | 2530-10N |
50 N Static Load Cell | .05 kN 11.2 lbf | 2.5 mm Clevis Pin with 6 mm Adapter (Type OOf & Of) | 2530-50N |
100 N Static Load Cell | .1 kN 22.5 lbf | 2.5 mm Clevis Pin with 6 mm Adapter (Type OOf & Of) | 2530-100N |
500 N Static Load Cell | .5 kN 112 lbf | 6.0 mm Clevis Pin (Type Of) | 2530-500N |
1 kN Static Load Cell | 1 kN 225 lbf | 6.0 mm Clevis Pin (Type Of) | 2530-1kN |
2 kN Static Load Cell | 2 kN 450 lbf | 6.0 mm Clevis Pin (Type Of) | 2530-2kN |
5 kN Static Load Cell | 5 kN 1125 lbf | 0.5 in Clevis Pin (Type Df) | 2530-5kN |
10 kN Static Load Cell | 10 kN 2250 lbf | 0.5 in Clevis Pin (Type Df) | 2530-10kN |
30 kN Static Load Cell | 30 kN 6750 lbf | 0.5 in Clevis Pin (Type Df) | 2530-30kN |
50 kN Static Load Cell | 50 kN 11250 lbf | 0.5 in Clevis Pin (Type Df) | 2530-50kN |
100 kN Static Load Cell | 100 kN 22500 lbf | 0.5 in Clevis Pin (Type Df) | 2530-100kN |
300 kN Static Load Cell | 300 kN 67500 lbf | M48 x 2LH (Type IIF), 6 off M20 on 150 PCD, 6 off M10 on 100 mm PCD | 2530-300kN |