ASTM D7137 measures the compression strength of multidirectional composite coupons which have been previously subjected to an indentation according to test method ASTM D6264/D6264M, or drop-weight impact in accordance with test method ASTM D7136/D7136M. ASTM D7137 is mainly used by the aerospace industry to produce compressive property data for material specifications, research and development, quality assurance, and structural design and analysis. 

Damage from out-of-plane forces is a major concern for design engineers working with composite materials. The impact portion of this test method simulates damage that the material is expected to incur in the field, such as a tool being dropped onto the surface of a plane during maintenance or a bird hitting the plane's wing. ASTM D7137 testing is important because the compressive strength of a composite plate is reduced even when an impact is not sufficient enough to cause visible damage. ASTM D7137 helps design engineers gain knowledge of the damage resistance and tolerance properties of composite plate. The desired test results are the ultimate compressive strength and the effective compressive modulus.  

Materials Testing System

The compression portion of ASTM D7137 should be performed on a high force universal testing system such as Instron's 5980 Series equipped with an an AlignPro fixture and a custom compression after impact fixture. The material must first be subject to ASTM D7136/D1736M testing on an impact system such as Instron's 9400 Series drop towers. Drop towers must have an anti-rebound device to prevent a secondary impact. 




ASTM D7137 Test Setup
1)5900 Series Universal Testing System
2)Bluehill Universal Software
3)2580 Series Load Cell
4)CP103712 Custom Test Fixture

 

ASTM D7137 compression testing damaged composite plates
Related Content

Composites Testing Brochure

Instron’s universal testing machines are designed to perform the most common types of testing used in the composites industry, including but not limited to in-plane tensile, through thickness tensile, interlaminar shear, compression in end, shear, or combined loading, and compression after impact.

Composite Test Fixture - Compression After Impact

 The “Boeing CAI” fixture is used to test the impact resistance of carbon and other fiber-reinforced polymer composite laminates.

High Force Universal Testing Machines Brochure

Instron's high force systems include electromechanical and high-capacity hydraulic testing systems for tension and compression applications. Force capacities range from 100 kN to 2000kN.

5980 Series Dual Column Floor Model

5980 floor models are robust, heavy-duty frames commonly used for testing high-strength metals and alloys, advanced composites, aerospace and automotive structures, bolts, fasteners, and plate steels.

AlignPRO Alignment System

Instron's AlignPROTM system is designed to assist machine operators when measuring and adjusting load string alignment.