ISO 1798 Tensile Strength Flexible Cellular Polymeric Materials
The ISO 1798 method determines the tensile and deformation properties of flexible cellular materials when extended at a constant rate of displacement until failure. These properties include tensile strength and elongation at break.
The challenges:
- Specimen gripping
- Repeatable strain measurements
- Reporting test results in compliance with the standard
Our solutions:
- Specimen gripping – Recommended gripping options include pneumatic side action grips and advanced screw action grips. Pneumatic side acting grips provide a constant clamping force to eliminate slippage and produce repeatable results.
- Repeatable strain measurements – Advanced strain solutions include non-contacting extensometers, such as the Advanced Video Extensometer (AVE2) and automatic contacting extensometers, such as the AutoX750. These solutions require little influence from the operator, resulting in improved repeatability. Contacting long travel extensometers also meet the measurement accuracy requirements of the standard.
- Reporting test results in compliance with the standard – Bluehill® Universal testing software offers advanced methods that are available with pre-configured calculations to ensure compliance with the reporting requirements of this standard.
It is important to review ISO 1798 to fully understand the test setup, procedure, and results requirements.
AVE 2 Non-Contacting Video Extensometer
The second generation Advanced Video Extensometer (AVE 2) utilizes patented measurement technology in the fastest, most accurate non-contacting strain measurement device commercially available.
- Products
- 1/26/2018
- 1.4 MB
AutoX750 Automatic Contacting Extensometer
The AutoX750 is a high-resolution, long-travel automatic contacting extensometer that is used to determine a variety of calculations including modulus, offset yield, plastic elongation to failure (non-proportional), and r and n values for sheet metals.
- Products
- 8/15/2013
- 1.3 MB
2630-080 Long Travel Extensometer
The Instron® model XL (long travel) extensometer is a precise device for measuring strain in highly extensible materials such as elastomers, semi-rigid plastics and films.
- Products
- 10/23/2018
- 151.4 KB
Pneumatic Side Action Grips 2712-04x Series
The 2712-04x Series Pneumatic Side Action grips are ideal for static tensile testing on a wide range of materials and specimen types including plastics, elastomers, metals, textiles, paper, thin sheet, foil, and wire.
- Products
- 3/22/2022
- 1.1 MB
2710-100 Series Screw Side-Action Grips
Screw side-action grips provide a very simple and efficient method for holding test specimens in a wide range of applications. The dual - acting design of 2710-100 series grips means that jaw faces can be adjusted to accommodate different specimen thicknesses. This ensures that the line of tensile force remains concentric with the grip body. They can be equipped with a selection of interchangeable grip jaw faces in various sizes and choice of surfaces including smooth ground, rubber-coated and serrated. Line contact and special coated faces are also available.The unique ‘snap-on’ jaw face attachment makes changing faces extremely quick and simple.
- Products
- 6/28/2017
- 1.3 MB
3400 Series Universal Testing Systems
Instron 3400 Series universal testing systems for tensile, compression, bend, and other material property tests.
- Products
- 1/27/2022
- 11.6 MB
6800 Series Universal Testing Systems
Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.
- Products
- 2/10/2020
- 3.6 MB
Bluehill® Universal Software
Bluehill Universal Software is built from the ground-up for touch interaction and an intuitive user experience. Discover simpler and smarter testing with features such as pre-loaded test methods, QuickTest in seconds, enhanced data exporting: and Instron Connect – a new feature that provides a direct communication link to Service. Users of previous versions of software such as Bluehill 2 and Bluehill 3 can easily upgrade to the newest version of Bluehill.
- Products
- 2/26/2017
- 4.4 MB