Fatigue Testing Stent Materials and Structures

The challenge

Traditional testing of stent and stent grafts (to standards such as ASTM F2477) involves subjecting complete devices to pressure pulsation simulating blood flow for a pre-specified number of cycles. Even if the device has not fractured, a simple pass/fail criterion is used for the test to succeed. Industry work is being undertaken to attempt to develop improved in vitro methods for characterizing and evaluating cardiovascular implant devices to provide more information about when and under what conditions fracture will take place.

To enable a representative sample of specimens to be evaluated and to reduce overall test time, multiple samples must be tested on a single system.



16 Station Carousel

Stent Systems Complete System Half in Bath

WaveMatrix2 Screen
Our SolutionThe ElectroPuls® 16-Station testing system was developed to assist cardiovascular implant manufacturers to assess this long-term fatigue characteristics of nickel-titanium (Nitinol) and stainless-steel stent materials and structures.

Each specimen station features a fatigue-rated load cell, precision alignment adjustment and grips that are unique to the material or structure undergoing test. The entire station assembly is submerged into a temperature controlled bath to test the specimens in vitro.

The test is controlled by WaveMatrix2 Dynamic Test Software that includes a number of features designed to assist users in running the test. These include integrated temperature control of the fluid bath, a live display of each load cell reading, and trend monitoring of forces to determine each specimen fracture.

Related Content

ElectroPuls® 16-Station Testing System

The Electropuls 16-Station testing system performs high cycle fatigue testing on multiple samples simultaneously, with a fatigue-rated load cell included on each station. The fixture uses a carousel designed with high stiffness and low mass to enable high frequency testing and reduce test time.

ElectroPuls® Brochure

ElectroPuls instruments are state-of-the-art electrodynamic test systems for dynamic and static tests on materials and components. Powered entirely from a single-phase mains supply, they feature the latest in testing technology and a host of other user-oriented features.

WaveMatrix2 Brochure

WaveMatrix2 is intelligent software designed for fatigue and dynamic testing of materials and components. It delivers flexibility - run everything from a simple static ramp, to cyclic waveforms through to complex multi-step, multi-axial tests The highly visual environment with integrated tabular screens, clear menu structures, time-based matrix test preview and configurable live test workspace is designed to be intuitive and instill confidence. Packed with intelligent features, such as data reduction and built-in project organization, designed to simplify your testing.