Bagley Correction
During capillary rheometer tests, pressure is measured above the die inlet. The true pressure drop along the capillary is therefore ‘hidden’ by an additional pressure drop at the entrance of the die, where the flowing material goes from a wide reservoir (the main cylinder or barrel) to a narrow capillary, possibly also creating turbulences. Assuming that the same additional pressure drop takes place with different capillary lengths (but keeping constant barrel and capillary diameter, and inlet shape), it’s possible to correct the pressure reading and estimate much more accurately the true pressure drop. This is called the Bagley correction (named after Edward B. Bagley, American scientist).
The simple pressure reading is used to calculate what is called an apparent shear stress, giving only an apparent viscosity value. Bagley correction gives a true shear stress, and the true viscosity can be calculated. True viscosity is a property of the material (varying with test temperature), and is comparable even if obtained with different rheometers and with different capillary dies. The correction is strongly recommended when the data is to be used for design, flow simulation or fundamental studies. On the contrary, apparent viscosity can only be used to compare different samples tested with the same instrument and die, and is typically used for quality control.
The Bagley correction requires at least two sets of data obtained with the same sample, same temperature, same barrel and capillary diameter, same capillary inlet, and different capillary lengths. The use of ‘zero-length’ dies is not recommended by international standards.
With a twin-bore capillary rheometer it is possible to get Bagley-corrected viscosity right at the end of a single test run, while the same result requires two tests with a single-bore machine.
References
- ISO 11443: 2005 “Determination of the fluidity of plastics using capillary and slit-die rheometers”
- ASTM D3835-09 “Standard Test Method for Determination of Properties of Polymeric Materials by Means of a Capillary Rheometer”
3400 Series - Affordable Testing Solutions
Instron 3400 Series Universal Testing Systems for Tensile, Compression, Bend, and other material property tests.
6800 Series Premier Testing Systems Brochure
Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.
Bluehill Universal Brochure
Bluehill Universal Software is built from the ground-up for touch interaction and an intuitive user experience. Discover simpler and smarter testing with features such as pre-loaded test methods, QuickTest in seconds, enhanced data exporting: and Instron Connect – a new feature that provides a direct communication link to Service. Users of previous versions of software such as Bluehill 2 and Bluehill 3 can easily upgrade to the newest version of Bluehill.