ASTM D1708-13 Tensile Properties of Plastics by Use of Microtensile Specimens

ASTM D1708 is a standardized test method to determine the tensile properties of plastic microtensile specimens. The tensile properties reported are yield stress, yield strain, tensile strength, break stress, and break strain. Modulus of elasticity shall not be determined when using D1708’s microtensile specimen.

 

ASTM D1708 microplastic tensile testing

ASTM D1708 is recommended for labs that have a historical material property data that was obtained through D1708 testing. If no such historical data exists, it is recommended to refer to ASTM D638 or ASTM D882. If material is limited for testing purposes, ASTM D638’s Type V specimen is similar in size to the microtensile specimen defined in D1708.

Plastic manufacturers must design plastic to meet the requirements of the end application. Whether they are supplying plastic to produce biomedical devices, bicycle helmets, or children toys, each application has specific strength requirements in addition to safety, weight, environmental resistance, and other requirements. Determining the tensile properties of a polymer provides useful strength and deformation data for the plastics engineering process. It is worth noting that the properties of plastics have a high sensitivity to the rate which rate they are pulled (tension) or pushed (compression). It is important to recognize this sensitivity as properties experienced in the end application can differ from those observed during a controlled test. For this reason, ASTM D1708 and other plastics testing standards are generally used for quality control in a production setting or for comparative purposes in a R&D setting.

Materials Testing System

As typical forces will not exceed 1 kN (225 lbf) and displacements will not exceed 2 inches (50 mm), we recommend a low force single column test frame such as those found in Instron's 3400 and 6800 series.




ASTM D1708 Test Setup
1) 6800 Series Universal Testing System
2) Bluehill Universal Software
3) 2580 Series Load Cell
4) 2712-041 pneumatic side action grips

 

ASTM D1708 plastic tensile testing

Grips

Due to the low forces involved, 250 N pneumatic side action grips (2712-052) or 1 kN manual wedge grips (2716-016) should be sufficient for most ASTM D1708 testing.

250 N Model | 2712-052
2616-017
2 kN Model | 2716-017

Tips and Tricks 

  • Gripping can be a challenge when testing subsized specimens. ASTM D1708 allows a minimum specimen shoulder length (the region of the specimen that is gripped) of 8 mm, which can cause difficulties due to insufficient specimen insertion into the grip’s jaw face. When insufficient specimen insertion exists, it is recommended to use grips that do not allow jaw face pivot as it can cause unwanted stress concentrations along the specimen. With sufficient specimen insertion, Instron recommends its 250 N capacity pneumatic side-action grips (2712-052) with serrated jaw faces. With insufficient jaw face insertion, Instron’s 1 kN capacity, manual wedge action grips (2716-016) are recommended.
  • Due to their small size, microtensile specimens can increase the chances of a pinch hazard when operators clamp the specimen with pneumatic grips. Instron’s 3400 and 6800 frames have an optional Smart-Close Air Kit that is fully integrated into the frame and software. The Smart-Close Air Kit minimizes pinch hazards by closing the jaw faces at a reduced speed and pressure during installation. When the test is ready to begin full pressure is applied, and the test routine starts.

Related Content

6800 Series Premier Testing Systems Brochure

Instron 6800 Series Universal Testing Systems provide unparalleled accuracy and reliability. Built on a patent-pending Operator Protect system architecture with an all-new Smart-Close Air Kit and Collision Mitigation features, the 6800 Series makes materials testing simpler, smarter, and safer than ever before.

3400 Series - Affordable Testing Solutions

Instron 3400 Series Universal Testing Systems for Tensile, Compression, Bend, and other material property tests.

Bluehill Universal Brochure

Bluehill Universal Software is built from the ground-up for touch interaction and an intuitive user experience. Discover simpler and smarter testing with features such as pre-loaded test methods, QuickTest in seconds, enhanced data exporting: and Instron Connect – a new feature that provides a direct communication link to Service. Users of previous versions of software such as Bluehill 2 and Bluehill 3 can easily upgrade to the newest version of Bluehill.

2712-05x Series Pneumatic Side-Action Grips

Pneumatic side-action grips offer a versatile gripping solution for a wide range of materials. Rated capacities up to 250 N.

2716-01x, 2716-02x, & 2736-01x Manual Wedge Grips