A derived channel is a test data channel calculated using data from the transducers that monitor the specimen. For example, stress is derived using load data from the load cell, average strain is derived by dividing the sum of two strain channels. Some derived channels are specific to the test type. For example, flexure stress is derived from load divided by an outer fiber stress factor.