Shear Fixture for Wood
2820-060 | Shear Fixture for Wood
Capacity: 50 kN (5,000Kgf, 11,250lbf).
Temperature Range: Ambient only
Upper Fitting: 0.5 in clevis (Type Dm)
Lower Fitting: 0.5 in clevis (Type Dm)
Features:
- Self-aligning loading anvil
- 0 mm, 2.0 mm and 3.0 mm clearance with shims provided
- Specimen clamp
Meets:
ASTM D 143-94, ASTM D 905-98, ISO 6238 2001, JIS K 6802-1973, JIS Z 2117-1977, BS 373: 1957 and JAS 601-1974 testing standards.
Accessory Weight | 11 kg (24 lb) |
---|---|
Accessory Width | 130 mm (5.1 in) |
Capacity | 50 kN (11,250 lbf) |
Lower Fitting | 0.5 in (Type Dm) |
Specimen Length | 63 (Typical) mm (2.5 (Typical) in) |
Specimen Thickness | 50 (Typical) mm (2 (Typical) in) |
Specimen Width | 50 (Typical) mm (2 (Typical) in) |
Testing Standards | ASTM D 143-94, ASTM D 905-98, ISO 6238 2001, JIS K 6802-1973, JIS Z 2117-1977, BS 373: 1957 and JAS |
Upper Effective Length | 350 mm (13.8 in) |
Upper Fitting | 0.5 in (Type Dm) |
Shear Test Fixture For Wood | 2820-060
The 2820-060 wood shear fixture is designed for testing shear strength properties of wood or adhesive bonds in wood by compression loading. The fixture consists of a high-strength steel body with a sliding, self-aligning anvil which is used to apply compressive loading to the specimen in shear. The shear line can be set at 0.0 mm, 2.0 mm or 3.0 mm by using shims. The shims are clearly engraved with the applicable standard and are easy and quick to change. The fixture is attached to the test system using simple clevis pin interfaces which allow quick and easy fitting and removal.