One (1) High Temperature Pull Rod, 273 mm (10.75 in) long, threaded 0.75-10m-RH both ends, made of Inconel 713-C.
Rated for 9070 kgs (20,000 lbs) load up to 760 Deg. C (1400 Deg. F) and 1360 kgs (3000 lbs) load at a maximum temperature of 1100 Deg. C (2000 Deg. F).
Common load train applications: for use on Model M3 Creep/Stress Rupture machines and in hot tensile load trains.
Accessory Length | 273 mm (10.75 in) |
---|---|
Capacity | 90 / 26.7 kN (20000 / 6000 lbf) |
Lower Fitting | 0.75 in-10mRH |
Material Type | 713C |
Static or Fatigue Rated | Static |
Temperature Rating | 538 / 1100°C (1000 / 2000°F) |
Upper Fitting | 0.75 in-10mRH |