Guided Bend and Weld Optional Loading Noses

The Weld Bend fixture can be used to test a variety of specimen thicknesses when equipped with optional loading struts. A separate loading strut is required for each thickness of specimen, several struts are available.The appropriate loading strut is attached to the adjustable crosshead using the grip bumper plate or a threaded adapter and the span of the base is adjusted to the correct position for the strut being used.

Principle Of Operation

The appropriate loading strut is attached to the adjustable crosshead using the grip bumper plate or a threaded adapter and the span of the base is adjusted to the correct position for the strut being used.

Application Range

The Weld Bend fixture can be used to test a variety of specimen thicknesses when equipped with optional loading struts. A separate loading strut is required for each thickness of specimen, several struts are available.