For Static Hydraulic and Pneumatic Wedge-Action Grips

This series of grip faces is designed to provide the best possible gripping for Instron 2716 Series, Static Hydraulic and Pneumatic Wedge Action Grips.

Not every face can be used to test every material. Variations of flat surfaces and grooved faces have been developed to accommodate a wider range of requirements. 

The faces are designed with serrations of 10, 20 or 25 teeth per inch for maximum gripping effectiveness.

Principle Of Operation

The faces are available with either flat or v-grooved surfaces and in a range of sizes to accommodate most types of specimen sizes and material types.

The 20 and 25 teeth per inch serrations are ideal for, thin, very hard, or penetration sensitive materials.

Application Range

  • Types of Loading: static tension 
  • Application Range: wires, metals 
  • Specimen Types: flat or round specimens

Accessories

Accessories
Item Name Cat #
Jaw Faces for Flats (Serrated, 0 - 15 mm) W-5191-A
Jaw Faces for Flats (Serrated, 0 - 15 mm) W-5181-A
Jaw Faces for Flats (Serrated, 0 - 20 mm) 16 TPI 2703-185
Jaw Faces for Flats (Serrated, 0 - 20 mm) 25 TPI 2703-180
Jaw Faces for Flats (Serrated, 0 - 30 mm) W-5197-A
Jaw Faces for Flats (Serrated, 0-16 mm) W-5246-A
Jaw Faces for Flats (Serrated, 15 - 30 mm) W-5181-B
Jaw Faces for Flats (Serrated, 15 - 30 mm) W-5191-B
Jaw Faces for Flats (Serrated, 16 - 32 mm) W-5246-B
Jaw Faces for Flats (Serrated, 20 - 40 mm) 16 TPI 2703-186
Jaw Faces for Flats (Serrated, 20 - 40 mm) 25 TPI 2703-181
Jaw Faces for Flats (Serrated, 30 - 45 mm) W-5191-C
Jaw Faces for Flats (Serrated, 30 - 45 mm) W-5181-C
Jaw Faces for Flats (Serrated, 30 - 60 mm) W-5197-B
Jaw Faces for Flats (Serrated, 32 - 50 mm) W-5246-C
Jaw Faces for Flats (Serrated, 45 - 60 mm) W-5191-D
Jaw Faces for Flats (Serrated, 45 - 60 mm) W-5181-D
Jaw Faces for Flats (Serrated, 60 - 70 mm) W-5191-E
Jaw Faces for Rounds (Vee-Serrated, 10 - 20 mm) W-5247-B
Jaw Faces for Rounds (Vee-Serrated, 10 - 35 mm) W-5198-B
Jaw Faces for Rounds (Vee-Serrated, 15 - 30 mm) W-5185-C
Jaw Faces for Rounds (Vee-Serrated, 15 - 30 mm) W-5195-C
Jaw Faces for Rounds (Vee-Serrated, 16 - 34 mm) 2703-183
Jaw Faces for Rounds (Vee-Serrated, 20 - 30 mm) W-5247-C
Jaw Faces for Rounds (Vee-Serrated, 3 - 10 mm) W-5198-A
Jaw Faces for Rounds (Vee-Serrated, 3 - 10 mm) W-5247-A
Jaw Faces for Rounds (Vee-Serrated, 3 - 5 mm) W-5195-A
Jaw Faces for Rounds (Vee-Serrated, 3 - 5 mm) W-5185-A
Jaw Faces for Rounds (Vee-Serrated, 30 - 40 mm) W-5247-D
Jaw Faces for Rounds (Vee-Serrated, 30 - 45 mm) W-5195-D
Jaw Faces for Rounds (Vee-Serrated, 30 - 45 mm) W-5185-D
Jaw Faces for Rounds (Vee-Serrated, 33 - 50.8 mm) 2703-184
Jaw Faces for Rounds (Vee-Serrated, 35 - 57 mm) W-5198-C
Jaw Faces for Rounds (Vee-Serrated, 45 - 60 mm) W-5195-E
Jaw Faces for Rounds (Vee-Serrated, 5 - 15 mm) W-5185-B
Jaw Faces for Rounds (Vee-Serrated, 5 - 15 mm) W-5195-B
Jaw Faces for Rounds (Vee-Serrated, 6 - 17.8 mm) 2703-182