In-Head Flat Wedge Jaws
W-1660 | In-Head Flat Wedge Jaws
Set of (4) wedge grip jaws for flat specimens from 0 to 76 mm (3 in) thick by up to 90 mm (3.5 in) wide.
Tooth Profile: Diamond cut, 8 TPI (teeth per inch)
Accessory Length | 171.5 mm (6.750 in) |
---|---|
Accessory Weight | 8.2 kg (18.00 lb) |
Accessory Width | 101.3 mm (3.988 in) |
Capacity | 1,500 kN (337,500 lbf) |
Compatible Frame Models | 5595, 300HVL |
Specimen Thickness | 76 mm (3.000 in) |
Specimen Width | 90 mm (3.500 in) |
Surface | Diamond |
Teeth Per Inch | 8 |