Tension-Only Holders, M8 Thread
3117-025 | Tension-Only Holders, M8 Thread For 3117-020/-021 Pullrods
- M8 Thread For 3117-020/-021 Pullrods.
- Maximum Capacity 10kN at 300 deg. C.
- Maximum Capacity 10kN at 800 deg. C.
- Maximum Capacity 7kN at 850 deg. C.
- Maximum Capacity 5kN at 900 deg. C.
- Maximum Capacity 3kN at 950 deg. C.
- Maximum Capacity 2kN at 1000 deg. C.