Lever Action, Mechanical Wedge Grips; Capacity: 150 kN
W-5151 | Lever Action, Mechanical Wedge Grips; Capacity: 150 kN
150 kN (15,000 kg, 33,750 lb) capacity T-Grip Bodies
- Set of 2
- Open front bodies
- Spring/lever actuated wedge grip jaws
- Specimen sizes; flats 0.016"- 1.0" thick x up to 2" wide and rounds 0.375" up to 1.0" diameter
- Bodies are tapped M36x4 female Right Hand thread
- Nominal weight per grip body is 35 lbs
- Approx. size : 6-1/2"H x 11"W x 4-1/2"D
- Jaws are listed as separate items
Accessory Height | 165.1 mm (6.5 in) |
---|---|
Accessory Width | 279.4 mm (11 in) |
Capacity | 150 kN (33,750 lbf) |
Lower Fitting | M36x4fRH |
Specimen Diameter | 9.5 - 25.4 mm (0.375 - 1.000 in) |
Specimen Thickness | 0.4 - 25.4 mm (0.016 - 1.000 in) |
Specimen Width | 50.8 mm (2.000 in) |
Upper Effective Length | 129.1 mm (5.1 in) |
Upper Fitting | M36x4fRH |
- Jaw Faces for Rounds (9.5 - 15.9 mm)
- Jaw Faces for Rounds (15.9 - 25.4 mm)
- Jaw Faces for Flats (0 - 12.7 mm)
- Jaw Faces for Flats (12.7 - 25.4 mm)