Pneumatic Wire Tire Cord Grips, Surfalloy, 5 kN
CP108524 | Pneumatic Tire Cord and Yarn Grips
Capacity: 5.0 kN (1,000 lb, 500 kg).
Incorporates a surfalloy coated clamping surface.
Temperature range: -10 °C to 80 °C (14 °F to 176 °F).
Maximum specimen diameter: 2 mm (0.08 in).
Upper and lower fittings: Type Dm (1.25 in connection with ½ in clevis pin).
Requires a rigid coupling and an Automatic Air Control Kit or Pneumatic Foot Switch
Accessory Weight | 4.54 kg (10 lb) |
---|---|
Accessory Width | 245 mm (9.6 in) |
Capacity | 5 kN (1125 lbf) |
Effective Length | 248 mm (9.76 in) |
Lower Fitting | 1/2 in clevis pin (Type Dm) |
Specimen Diameter | 2 mm (0.07 in) |
Temperature Rating | -10 to + 80°C (+14 to +176°F) |
Upper Fitting | 1/2 in clevis pin (Type Dm) |
2714 Series Pneumatic Tire Cord Grips (2714-010/CP108524)
The Instron® pneumatic tire cord grips provide a convenient method for clamping tire cord and braided wire during testing. A guide pin allows for easy loading onto a graduated radius cam, which provides a stress-reduced clamping area on the specimen. The clamping mechanism can be activated either automatically or through a footswitch, which allows for hands-free grip operation enabling the specimen to be held with both hands for easy loading. Pneumatic cord and yarn grips provide selectable clamping force to accommodate different materials and excellent follow-up action that compensates for decay of the holding force due to specimen creep.
- Productos
- 8/14/2013