Instrumented Charpy Striker 8 mm Radius
Instrumented Charpy Impact Striker, 8 mm Radius, Heavy Duty
Capacity 89 kN (20,000 lbs)
For use on Retrofitted SI Series, and MPX Series Pendulum Machines
Compliant with ASTM E23
Requires Impulse Software
Replaces 7900-810 & 7900-820