Capillary Rheometer

A capillary rheometer is an apparatus designed to measure shear viscosity and other rheological (= flow) properties. Capillary rheometers for plastics are piston-die systems designed to measure viscosity of polymer melts as a function of temperature and rate of deformation. They are capable of testing basic polymers, compounds, various composites with small reinforcing particles or fibers, feedstock for metal injection molding and similar materials.

The basic principle is that a thermoplastic sample (originally in the shape of granules, powder or flakes) is made fluid by heating and forced to flow out of a cylinder through a capillary die. The measured quantity is normally the generated pressure under steady state conditions. A flow curve is the typical output, obtained by interpolation of several experimental data. Viscosity is represented as the Greek letter “eta” (η) and expressed (in SI units) in pascal seconds (Pa·s) or newton seconds per square meter (N·s/m2).

Capillary rheometers ensure testing conditions which are truly representative of processing conditions, especially for high-pressure and high-speed techniques like injection molding, therefore they are key for process optimization.

Other rheological properties that can be measured or estimated from capillary rheometers data include extensional viscosity, extrudate swell, thermal stability, wall slip. Ancillary measurements can be carried out for thermal conductivity, density dependence on pressure and temperature (pvT), melt strength.

References

  • Walters K. “Rheometry”, Chapman & Hall (1975)
  • Ferry, J. D. “Viscoelastic Properties of Polymers”, John Wiley & Sons (1980)
  • Dealy, J.M. and Wissbrun K.F. “Melt Rheology and its Role in Plastics Processing”, Van Nostrand Reinhold (1990), Chapman & Hall (1995)
  • Macosko C.W. “Rheology – Principles, Measurements, and Applications”, Wiley-VCH (1994)
  • Malkin A.Y. “Rheology – Concepts, Methods, & Applications”, ChemTec Publishing (2006)
Related Content

Serie 3400: soluciones de ensayo asequibles

Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.

Catálogo de sistemas de ensayo Serie 6800 Premier

Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.

Catálogo de Bluehill Universal

El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.

Contacto

Contacto

Para obtener más información sobre nuestra industria y nuestras soluciones de pruebas, póngase en contacto con nosotros. Nuestros equipos de atención al cliente están listos para ayudarle.