Offset Yield Strength

Offset yield strength is an arbitrary approximation of a material's elastic limit. It is the stress that corresponds to a point at the intersection of a stress-strain curve and a line which is parallel to a specified modulus of elasticity line. This parallel line is horizontally offset by a predetermined amount. The intersection point represents the yield point of the material being tested. The value of the offset (expressed as a percentage of strain) is arbitrarily defined by the material testing standard (ASTM or ISO) being used. The most common offset is 0.2%, but this can vary depending on the material. By the time the material reaches its offset yield point, it usually will have surpassed its elastic limit and experienced a small percentage of plastic strain approximately equivalent to the offset value. The testing industry has accepted this standardized approach as one method to determine the yield strength of materials that do not have an easily discernible yield point.

How is Offset Yield Strength Different from Elastic Limit?

The elastic limit is the greatest stress that can be applied to a material without causing plastic deformation. The offset yield point differs from the elastic limit, as offset yield will generally occur beyond the material's elastic limit.

How is Offset Yield Strength Different from Proportional Limit?

The proportional limit is the point on a stress-strain curve where the linear, elastic deformation region transitions into a non-linear, plastic deformation region. Offset yield strength differs from the proportional limit as offset yield can be beyond a material's linear region.

proportional limit illustration

Related Content

Serie 3400: soluciones de ensayo asequibles

Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.

Catálogo de sistemas de ensayo Serie 6800 Premier

Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.

Catálogo de Bluehill Universal

El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.

Contacto

Para obtener más información sobre nuestra industria y nuestras soluciones de pruebas, póngase en contacto con nosotros. Nuestros equipos de atención al cliente están listos para ayudarle.