Tensile Impact Test with Pendulum Impact Tester
What is a Tensile pendulum impact test?
A test method for determining energy required to fracture a specimen under shock tensile loading. Typically executed on a pendulum testing machine, the tensile impact strength test was originally developed to overcome the deficiencies of flexural (both Izod and Charpy) impact test. All the test variables that have a high effect on the results, such as notch sensitivity, toss factor and specimen thickness, are eliminated in the tensile impact test. This test, on the contrary of Izod and Charpy types, which are limited to thick specimen only, allows to determine the impact strength of very thin and flexible specimens.How is a Tensile pendulum impact test performed?
There are two different test configurations. One consists in a specimen-in-head kind of setup (ISO 8256 method B), where the specimen is attached directly to the pendulum hammer. The energy to break by impact is determined by the kinetic energy value extracted by the pendulum in the process of breaking the specimen. The test setup requires to mount one end of the specimen on the hammer and the other end has to be gripped inside a crosshead member, which travels together with the pendulum until the impact instant. As long as the machine bas is rigid enough to prevent vibrations, the energy lost by the bounce of the crosshead in the opposite direction can be easily calculated.The second test configuration is a specimen-in-base setup (ISO 8256 method A). The specimen is clamped in a specimen vice supported by the frame of the pendulum and it is broken by the impact between pendulum and crosshead member, which is always clamped on the other extremity of the specimen.
The following figure illustrates the most common specimen-in-base impact configuration.
Serie 3400: soluciones de ensayo asequibles
Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.
Catálogo de sistemas de ensayo Serie 6800 Premier
Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.
Catálogo de Bluehill Universal
El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.