ASTM D1414 Standard Test Methods for Rubber O-Rings
- Elastomers
- Tension
- ASTM 1414
ASTM D1414 specifies the procedures for determining the physical properties of o-rings. O-rings are typically made of elastomeric material and are used to seal connections in pipes, tubes, etc. This testing standard is commonly used in the safety-critical aerospace, automotive, and consumer products industries.
Materials Testing SystemThough system capacity will depend on the strength of the elastomer, most tests to this standard will fall in the low-force range, making this application perfect for a single column frame such as Instron's 68SC or 34SC. The standard specifies a fixture consisting of two spools to hold an o-ring while under test. Instron’s 2717 Series elastomeric o-ring test fixtures were designed to accurately meet the requirements, and conveniently avoid the need for lubricants or external power motors. Designed for testing elastomeric materials in the form of rings, these fixtures avoid local stress concentrations by using a lower spindle that is rotated by a toothed belt driven from the moving crosshead. The upper spindle rotates freely, and the rotation frequency of the lower spindle is easily selected by moving the toothed belt from one pulley to another. When testing straight specimens or single strands, pneumatic side action grips with serrated or rubber coated faces are the preferred gripping configuration. The constant gripping force prevents specimen slippage while under test.
ASTM D1414 Test Setup | |
---|---|
1) | 6800 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2580 Series Load Cell |
4) | 2717 Series O-Ring Fixture |

- Due to the geometry of o-rings and the unique fixture needed to test them, standard stress (F/A) and strain calculations (∆L/Lo) do not apply. Consideration needs to be made for the fixture geometry (spool separation and diameter) as well as specimen geometry.
- Bluehill Universal is provided with one free application module upon purchase. Each module contains pre-configured test methods and supporting documentation to assist with testing to various standards, including ASTM D1414, which is part of the Elastomers module.
- The Expression Builder within Bluehill Universal software allows for custom calculations and results in order to adhere to the standard.
- To review the test methods in full, purchase ASTM D1414.
6800 Catálogo de sistemas de ensayo Serie Premier
Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.
Serie 3400: soluciones de ensayo asequibles
Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.
Catálogo de Bluehill Universal
El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.
Mordazas neumáticas de acción lateral Serie 2712-04X
Las mordazas neumáticas de acción lateral ofrecen una solución de agarre versátil para una amplia gama de materiales. Capacidades nominales entre 1 y 10 kN.