ASTM D1876 Peel Resistance for Adhesives, T-Peel Test
ASTM D1876 measures the comparative peel properties of adhesive bonds between flexible adherends by using a T-peel test. The test is referred to as a “T-peel” due to the shape the two flexible adherends form as they are pulled apart. Average peel strength for each specimen type and average, minimum, and maximum peeling loads for each individual specimen are the primary results of interest. Manufacturers use this standard for quality control in a wide range of industries as it is primarily intended for determining relative peel resistance between individual specimens or different types of adhesives. Direct comparison of different adhesives can only be made when specimen construction and test conditions are identical.
- Adhesives
- Tension
- Peel, Tear, Friction
- ASTM D1876
For peel tests, it is critical to use a high data acquisition rate to register all peaks and troughs in the data. Insufficient bandwidth may overlook important test events and lead to artificially low peel strength values. For this reason we recommend an Instron 6800 series test frame, which enables a data capture rate of up to 5 kHz. The ASTM D1876 standard states that the maximum specimen load should fall between 15%-85% of the maximum frame capacity, in most cases making a single column frame (68SC) with capacity of 5 kN or less ideal. If the adhesive requires a higher capacity system, Instron’s dual column table model frames are available up to 50 kN.
ASTM D1876 Test Setup | |
---|---|
1) | 6800 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2580 Series Load Cell |
4) | 2712-041 (1 kN) Pneumatic Side-Action Grips |

Pneumatic side action grips prevent specimen slippage by maintaining a constant clamping pressure throughout testing. They are available in capacities from 50N to 10kN, appropriate for the full range of adhesive strengths. Both advanced side action grips and pneumatic grips feature quick-change jaw faces that can be easily changed to accommodate different materials.
- When testing to ASTM D1876, the two adherends do not need to be the same material or thickness. However, if one adherend is more flexible than the other, attach the less flexible one to the moveable (top) grip.
- Bluehill Universal software comes with with one free application module upon purchase. Each module contains pre-configured test methods and supporting documentation to assist with testing to various standards. ASTM D1876 is included as part of the Adhesives module.
It is important to review ASTM D1876-08(2015)e1 in order to fully understand the test setup, procedure, and results requirements.
Related Content
6800 Catálogo de sistemas de ensayo Serie Premier
Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.
Serie 3400: soluciones de ensayo asequibles
Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.
Catálogo de Bluehill Universal
El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.
Mordazas neumáticas de acción lateral Serie 2712-04X
Las mordazas neumáticas de acción lateral ofrecen una solución de agarre versátil para una amplia gama de materiales. Capacidades nominales entre 1 y 10 kN.
Mordazas neumáticas de acción lateral Serie 2712-05x
Las mordazas neumáticas de acción lateral ofrecen una solución de agarre versátil para una amplia gama de materiales. Capacidades nominales de hasta 250 N.
Serie 2710 Mordazas de acción de tornillo
Las Mordazas de acción de tornillo proporcionan un método sencillo y eficaz para sujetar muestras de ensayo en una amplia gama de aplicaciones.