ASTM D3163: Lap-Shear Testing of Bonded Rigid Plastics

Written by Meredith Bernstein

ASTM D3163 is a tensile test used to measure the adhesive lap-shear strength of bonded rigid plastics.This testing standard is very similar to ISO 4587 and EN 1465, with the difference being that ASTM D3163 is used specifically to test adhesives applied to rigid plastics. To perform this test, a shear stress is applied to the specimen at a rate of 8.3 to 9.7 MPa per minute and the breaking force and shear strength are reported.

 

 Materials Testing System

System capacity will depend on the strength of the adhesive, however most tests to this standard will fall in the capacity range between 1 kN and 5 kN, making this application perfect for a single column frame (34SC or 68SC). If the adhesive requires a higher capacity system, Instron’s dual column table model frames are available up to 50 kN.

ASTM D3163 test setup

ASTM D3163 Test Setup

1. Instron 68SC-1

2. Bluehill Universal Dashboard (2490-696)

3. 2580 Series Load Cell (2580-1kN)

4. 1 kN Screw Side-Action Grips (2710-113)

 

 

Grips

Both pneumatic side-action grips and advanced screw side-action grips are excellent fixture choices for this standard. Both types of grips are adjustable in order to offset the jaw faces and ensure that the lap joint remains centered in the grips, and both feature quick-change jaw faces that can be easily changed to accommodate different materials.

5 kN Model | 2712-045
1 kN Model | 2710-113
Software

Bluehill Universal is provided with one free application module upon purchase. Each module contains pre-configured test methods and supporting documentation to assist with testing to various standards, including ASTM D3163 which is part of the Adhesives module.

Tips and Tricks
  • It is critical when testing lap joints that the centerline of the grips be directly aligned with the plane of the adhesive bond. This ensures a true shear force application to the adhesive. Offset jaw faces are necessary to achieve this test setup.
  • The standard requires reporting the breaking force or strength, however it’s important to remember that the shear strength is calculated by dividing the breaking force by the adhesive bond area.
Related Content

6800 Catálogo de sistemas de ensayo Serie Premier

Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.

Serie 3400: soluciones de ensayo asequibles

Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.

Catálogo de Bluehill Universal

El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.

Mordazas neumáticas de acción lateral Serie 2712-04X

Las mordazas neumáticas de acción lateral ofrecen una solución de agarre versátil para una amplia gama de materiales. Capacidades nominales entre 1 y 10 kN.

Serie 2710 Mordazas de acción de tornillo

Las Mordazas de acción de tornillo proporcionan un método sencillo y eficaz para sujetar muestras de ensayo en una amplia gama de aplicaciones.