ASTM D5961 - Bearing Response of Polymer Matrix Composite Laminates
- Composites
- Tension
- Compression
- Shear
- ASTM D5961
ASTM D5961 is a testing standard that covers the bearing response of pinned or fastened joints of composite laminates. Connecting individual composite components with rivets or fastener is a common solution for connection of parts in the aerospace industry. ASTM D5961 is used by material designers to determine material specifications for research and development, quality assurance, and structural design analysis.
Test MethodsASTM D5961 includes four different testing procedures: A, B, C, and D. Procedure A is designed for double-shear tensile loading on a single piece specimen. Procedure B is for single-shear tensile or compressive loading on a two piece specimen. Procedure C is for single shear tensile loading of a single piece specimen, and Procedure D is for double-shear compressive loading on a single piece coupon. The composite coupons are supposed to be balanced and symmetric with respect to their test direction.
It is important to note that these four testing procedures will give results that are not directly comparable. Due to the larger fastener rotation and higher peak bearing stress Procedure C will yield higher strengths than Procedure B. For protruding head fasteners Procedure D will most likely yield higher bearing results than Procedure C. Procedures A and C produce very similar results.
Materials Testing SystemASTM D5961 testing is best performed on a high force floor model such as Instron's 5980 Series equipped with either precision manual (2716-028/030) or hydraulic (2743-401)wedge grips for gripping the loading plates. This standard requires different loading tools for each procedure, usually involving loading plates, pins, and/or fasteners. A set of Grips is needed to grip the loading plates.
ASTM D5961 Test Setup | |
---|---|
1) | 6800 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2580 Series Load Cell |
4) | 2716-028/030 Precision Manual Wedge Grips |

Modelo de suelo de doble columna Serie 5980
Los modelos de suelo 5980 son bastidores robustos y resistentes que se utilizan de forma habitual para probar metales y aleaciones de alta resistencia, materiales compuestos avanzados, estructuras aeroespaciales y automotrices, pernos, fijadores y chapas de acero.
Catálogo sobre ensayos en materiales compuestos
Catálogo de máquinas de ensayo universales de alta fuerza
Los sistemas de alta fuerza de Instron incluyen sistemas de ensayo electromecánicos e hidráulicos de alta capacidad para aplicaciones de tensión y compresión. Las capacidades de fuerza van de 100 kN a 2000kN.
Mordazas de cuña de alta precisión 2716
Disponibles para 100 y 250 kN, las mordazas de cuña de alta precisión 2716-028/30 de Instron proporcionan un agarre fiable para una amplia gama de materiales, así como un ajuste repetible que cumple con los requisitos Nadcap.
2743-401 Mordazas de cuña hidráulicas
Las mordazas de cuña hidráulicas de 100 kN de Instron proporcionan una solución innovadora para realizar ensayos de alta capacidad y mejorar el rendimiento del agarre, la facilidad de uso y la seguridad del operario.