ASTM E290 Bend Testing of Material for Ductility

ASTM E290 bend testing of metals

ASTM E290 describes the testing requirements used to determine the ductility of metals through bend testing. Bend testing helps provide a visual indication of the material's ductility. ASTM E290 is divided into four methods for bending the specimen:

  • Guided Bend
  • Semi-Guided Bend
  • Free-Bend
  • Bend and Flatten.

These tests are performed by supporting the two ends of a specimen while loading it at the center with a mandrel or plunger. The test is completed when the designated angle of the bend, or other specified condition, has been reached. Afterwards, the specimen is visually inspected for cracks or defects, and failure is determined by the size of the cracks and imperfections allowed by the material specification.

Materials Testing System

For ASTM E290 testing we recommend using an Industrial Series DX or HDX model with Bluehill Universal software and a W-6810 test fixture. This fixture allows for adjustment of the support span and is supplied with various sizes of loading mandrels to accommodate different specimen thicknesses. The loading supports are held together with two tie rods to provide extra stiffness during loading. The DX or HDX Model dual test space load frames allow the bend test fixture to be positioned in the lower compression test space. Any tensile testing can also be accomplished in the upper tensile test space.




ASTM E290 Test Setup
Instron 1000 HDX
W-5340 Hydraulic Wedge Action Grips
W-6810 test fixture

 

ASTM E290 bend testing of metals
Related Content

Catálogo de máquinas de ensayo universales de alta fuerza

Los sistemas de alta fuerza de Instron incluyen sistemas de ensayo electromecánicos e hidráulicos de alta capacidad para aplicaciones de tensión y compresión. Las capacidades de fuerza van de 100 kN a 2000kN.

Modelos HDX de la Serie Industrial

Estos bastidores hidráulicos, con un espacio de ensayo doble y una pista de ensayo larga, están disponibles en capacidades de 1.000 kN (225.000 lbf) y 1.500 kN (337.500 lbf).

Catálogo de Bluehill Universal

El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.