ASTM F1306 Slow Rate Penetration Resistance of Flexible Barrier Films and Laminates
- Thin Films
- Compression
- ASTM F1306
ASTM F1306 specifies the test conditions for determining the characterization of flexible barrier films and laminates for slow rate penetration resistance to a driven probe at room temperature. The required calculations for this standard consist of peak force to break, energy to break, and probe penetration from initial contact to break.
The ability to characterize penetration resistance is critical for end-use performance of thin, flexible materials where a sharp object can damage the barrier’s protection. ASTM F1306 testing is common in the packaging industry, which supplies thin films to the food and consumer product sectors. Another relevant industry is battery production, which is interested in quantifying the puncture resistance of the separator films found in their Li-ion batteries.
ASTM F1306 Test SetupForce requirements of ASTM F1306 are generally lower than 250 N, making it appropriate for Instron's single column low force testing systems such as the 34SC-1 or 68SC-1, with load cells of 50 N, 100 N, or 500 N capacity. Instron's S1-14110 is a custom fixture made specifically for ASTM F1306 testing and can be ordered through our custom solutions group.ASTM F1306 Test Setup | |
---|---|
1) | 6800 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2580 Series Load Cell |
4) | S1-14110 Custom Puncture Fixture |

When comparing results with other laboratories, it is important to note that the diameter of the test probe, as well as the sample test diameter, will impact load and penetration values. The ASTM F1306 standard recommends a 3.2 mm diameter hemispherical probe and a sample test diameter of 34.9 mm.
Related Content6800 Catálogo de sistemas de ensayo Serie Premier
Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.
Serie 3400: soluciones de ensayo asequibles
Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.
Catálogo de Bluehill Universal
El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.