EN 12242 Peel Strength Touch and Close Fasteners (Hook and Loop)
- Textiles
- Tension
- Peel
- EN 12242
EN 12242 is a test method used to determine the peel strength of a touch and close (also known as “hook and loop”) fastener. A touch and close fastener is made up of two different types of materials: the male material is constructed with monofilament warp ends and finished to form-locking elements of either “hook” or “mushroom” shape. The female material is constructed with multifilament yarns in “loops”. When the two types of material are pressed together, the male and female elements engage to form a secure closure which can be separated by a peeling action from either end.
EN 12242 is widely used in the textile industry to evaluate different hook and loop fasteners. These fasteners have a wide range of uses, from apparel and footwear to consumer products to more industrial usage. In all cases, a complete understanding of their properties are important to ensure they perform as expected. The primary results of interest are minimum, maximum, and average peel strength.
Materials Testing SystemSystem capacity will depend on the strength of the fasteners. However, most tests to EN 12242 will fall in the 1 kN and 5 kN capacity range, making this application perfect for a single column frame such as Instron's 34SC or 68SC. Optimal gripping solutions include pneumatic side action and advanced side action grips, both of which feature quick-change jaw faces that can be easily changed to accommodate different materials as needed. Rubber-coated jaw faces are well suited to testing hook and loop fasteners.
EN 12242 Test Setup | |
---|---|
1) | 6800 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2580 Series Load Cell |
4) | 2710 Series Advanced Side Action Grips |

For peel tests, it is critical to use a high data acquisition rate to capture all peaks and troughs to ensure all test events are fully represented in the results. Too low of a bandwidth may “dull” the results and lead to artificially low peel strength values. Instron’s 6800 series frames enable a data capture rate of up to 2.5kHz. With the Bluehill Universal Advanced Performance option, data acquisition rate can be increased to 5 kHz.
6800 Catálogo de sistemas de ensayo Serie Premier
Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.
Serie 3400: soluciones de ensayo asequibles
Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.
Catálogo de Bluehill Universal
El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.
Mordazas neumáticas de acción lateral Serie 2712-04X
Las mordazas neumáticas de acción lateral ofrecen una solución de agarre versátil para una amplia gama de materiales. Capacidades nominales entre 1 y 10 kN.
Serie 2710 Mordazas de acción de tornillo
Las Mordazas de acción de tornillo proporcionan un método sencillo y eficaz para sujetar muestras de ensayo en una amplia gama de aplicaciones.