EN 2597 Carbon Fiber Reinforced Plastics. Unidirectional Laminates. Tensile Test Perpendicular to the Fiber Direction.

composites test and airplane

EN 2597:1998 is a testing standard that specifies the method of determination of the ultimate tensile strength, tensile modulusPoisson’s ratio, and strain at failure in tension of carbon fiber reinforced plastics in the form of unidirectional laminates. EN 2598 is used for product development and quality control by a range of manufacturers who use carbon fiber laminates, including the aerospace, automotive, wind energy, and construction industries. This method is only applicable to specimens where the axis is perpendicular to the direction of the fibers. Testing when the axis is parallel to the fiber direction calls for the use of EN 2561.

Materials Testing System

The strength of composite specimens with fibers oriented perpendicular to the loading direction (axis) are normally much lower than the strengths of specimens where the fibers are oriented in the loading direction. Hence, the test forces are much lower. However, since testing to EN 2597 is normally combined with a range of other, higher force tests on composite materials, an electromechanical floor model testing machine such as Instron's 5980 Series will be the most suitable solution. The large (1000:1) force measurement range of the 5980 means that both high and low force tests can be carried out without the need to change load cells. A table model electromechanical machine may have sufficient capacity for testing lower strength materials, such as glass fiber.




EN 2597 Test Setup
1) 5900 Series Universal Testing System
2) Bluehill Universal Software
3) 2580 Series Load Cell
4) 2742 Series Hydraulic Wedge Grips
5) AVE2 Non-Contacting Extensometer

 

EN 2561 test setup
Grips

Moving body grips meet the requirements of the standard and are available in both manually and hydraulically operated configurations. 


Catalog no. 2743-401

Catalog no. 2716-002



EN 2597 Testing Accessories
1)Strain Gauge 
2)Biaxial Clip-On Extensometer
3)Environmental Chamber

 

Testing Accessories

Strain measurement devices include strain gauges and extensometers. Strain gauges can be connected to the testing machine via easy-to-use strain gauge adapters. A range of suitable contacting extensometers for axial and bi-axial strain measurements are available. When strain at failure is required, a non-contacting strain measurement solution such as Instron's AVE2 is preferred. When tests need to be conducted at high or low temperatures, a temperature chamber along with grips capable of operation inside the chamber are required. 


strain gauge exensometer, biaxial extensometer, environmental chamber

Testing Tips and Tricks
  • Obtaining consistent results when testing composites requires accurate alignment of the test specimen. Instron testing frames and accessories provide excellent alignment.
  • Bluehill Universal software comes provided with one free applications module upon purchase. The composites module includes a pre-defined EN 2597 test method.
  • To read the test method in full, purchase EN 2597:1998
Related Content

Modelo de suelo de doble columna Serie 5980

Los modelos de suelo 5980 son bastidores robustos y resistentes que se utilizan de forma habitual para probar metales y aleaciones de alta resistencia, materiales compuestos avanzados, estructuras aeroespaciales y automotrices, pernos, fijadores y chapas de acero.

Catálogo de Bluehill Universal

El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.

Catálogo sobre ensayos en materiales compuestos

Las máquinas de ensayo universales de Instron están diseñadas para realizar los tipos de ensayos más comunes utilizados en el sector de los materiales compuestos, incluyendo, entre otros, tracción en plano, tracción a través de espesor, cizallamiento interlaminar, compresión en extremo, cizallamiento o carga combinada y compresión después de impacto.

Extensómetro de vídeo sin contacto AVE 2

La segunda generación del extensómetro de vídeo avanzado (AVE 2) utiliza la tecnología de medición de deformación sin contacto más rápida y precisa disponible en el mercado.

Extensómetros Serie 2630

 La serie 2630-100 de extensómetros ofrece velocidad de fijación y facilidad de uso. El diseño ligero y robusto de la estructura transversal elimina los errores causados por la distorsión física, mientras que la protección integrada garantiza que no se produzcan daños por la sobreextensión.

 Extensómetros de tipo Clip-on biaxiales y axiales de promedio

Los extensómetros de tipo Clip-on biaxiales y axiales de promedio de Instron están fabricados con aluminio de alta resistencia, titanio y acero inoxidable y utilizan galgas extensiométricas para la medición. 

Cámara ambiental Serie 3119-600

La cámara ambiental de la serie 3119-600 permite a los laboratorios realizar ensayos seguros y eficaces en una amplia gama de temperaturas no ambientales. 

Adaptadores para extensómetros

Desde el sector aeroespacial hasta el de la construcción, los extensómetros se utilizan en diversos sectores para medir la tensión en los materiales y las pruebas estructurales. Estos adaptadores para extensómetros permiten utilizar un solo extensómetro con cualquier canal extensométrico estándar de Instron.