EN 868-5 Materiales de Envasado Bolsas y Rollos Sellables de Lámina de Plástico

BS EN 868-5 peel test of medical packaging

EN 868-5 characterizes the seal strength of single-use sterilized medical packaging. This standard specifically focuses on packaging materials and systems for medical devices which need to be sterilized. The seal strength identifies the adhesion strength between the two materials of the packaging; typically, a coated paper backing, and a plastic film overlay. This standard is technically equivalent to ASTM F88 with minor differences in the specimen preparation and test procedure.

While packaging can span many industries, The seal strength of medical packaging is extremely important for two reasons – first to ensure that the packing can be opened easily by the medical professional, and second to ensure that the adhesive is strong enough to prevent any breaches of the packaging prior to their use. During shipping and storage the adhesive must remain viable to maintain sterilization: any breach in the packaging would desterilize the product potentially leading to life threatening infections for the patient.

EN 868-5 Test SetupEN 868-5 can be performed on an Instron 3400 or 6800 Series single column universal testing system with a 500 N load cell.



EN 868-5 Test Setup
1) 3400 Series Universal Testing System
2) Bluehill Universal Software
3) 2530 Series Load Cell
4) 2710-112 Screw Side Action Grips

 

EN 868-5 peel test of sterile medical packaging
Grips

When testing an adhesive to a thick substrate, standard grips result in a misaligned specimen. Testing to EN 868-5 requires either advanced screw side action grips or pneumatic side action grips, both of which can be adjusted to offset to ensure that the specimen remains centered in the load string. Pneumatic grips provide an advanced solution by ensuring a repeatable gripping force to eliminate slippage specimen slippage. Both options can be fitted with specimen centering devices to ensure proper alignment for each test, and both employ a patented “quick-change” jaw face design which enables operators to easily change jaw faces to accommodate the needs of their materials. Rubber-coated grip faces should be used so as to avoid tearing the delicate specimen. Jaw faces are available in many different sizes and are easily interchangeable. 

250 N Model | 2712-052
2710-112
500 N Model | 2710-112
Tips and Tricks

The specimen width and test speed are different than ASTM F88, but produce statistically similar results when the data is normalized.

Related Content

6800 Catálogo de sistemas de ensayo Serie Premier

Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.

Serie 3400: soluciones de ensayo asequibles

Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.

Catálogo de Bluehill Universal

El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.

Mordazas neumáticas de acción lateral Serie 2712-04X

Las mordazas neumáticas de acción lateral ofrecen una solución de agarre versátil para una amplia gama de materiales. Capacidades nominales entre 1 y 10 kN.

Serie 2710 Mordazas de acción de tornillo

Las Mordazas de acción de tornillo proporcionan un método sencillo y eficaz para sujetar muestras de ensayo en una amplia gama de aplicaciones.