Dynamic Extensometer 12.5mm GL ±2.5mm Travel
2620-602 | Dynamic Extensometer 12.5mm GL ±2.5mm Travel
Dynamic Extensometer for direct strain measurement and closed loop strain control. suitable for tensile, compressive & fatigue testing, the extensometer has a 12.5mm gauge length with a travel of ±2.5mm giving ±20% strain.
It includes a 12.5mm extender to give a gauge length of 25mm and ±10% strain and a 37.5mm extender to give a gauge length of 50mm and strain of ±5% strain.
Temperature range: -80C to +200C. Compatible with 8800 and 8500Plus controllers. May be immersed in acetone, silicone or alcohol.
Accessory Height | 56 mm (2,21 in) |
---|---|
Accessory Weight | 0,02 kg (0,044 lb) |
Accessory Width | 21 mm (0,83 in) |
Gauge Length | 12,5 ; 25 et 50 mm (0.49, 0.98 et 1.97 in) |
Specimen Diameter | 3 - 25 mm (0,12 à 1 in) |
Specimen Thickness | 3 - 12,5 mm (0,12 - 0,5 in) |
Specimen Width | 0 - 25 mm (0 - 1 in) |
Static or Fatigue Rated | Fatigue |
Temperature Rating | -80 à +200°C (-112 à +392°F) |
% Travel (Axial) | ±20, ±10 et ±5% |
2620 Series Dynamic Strain Gauge Extensometer
Wide operating temperature range, from -80 °C to 200 °C (-112 °F to 392 °F) Designed to meet the requirements of ISO 9513, BS 3846 and ASTM E 83
- Productos
- 1/5/2005
- 2.6 MB
2620-600 Series Dynamic Strain Gauge Extensometers - Reference Manual
This guide provides instructions on how to use your system components and controls, procedures for setting limits, calibration and other frequently performed operating tasks.