ASTM D1708-13 Tensile Properties of Plastics by Use of Microtensile Specimens

ASTM D1708 is a standardized test method to determine the tensile properties of plastic microtensile specimens. The tensile properties reported are yield stress, yield strain, tensile strength, break stress, and break strain. Modulus of elasticity shall not be determined when using D1708’s microtensile specimen.

 

ASTM D1708 microplastic tensile testing

ASTM D1708 is recommended for labs that have a historical material property data that was obtained through D1708 testing. If no such historical data exists, it is recommended to refer to ASTM D638 or ASTM D882. If material is limited for testing purposes, ASTM D638’s Type V specimen is similar in size to the microtensile specimen defined in D1708.

Plastic manufacturers must design plastic to meet the requirements of the end application. Whether they are supplying plastic to produce biomedical devices, bicycle helmets, or children toys, each application has specific strength requirements in addition to safety, weight, environmental resistance, and other requirements. Determining the tensile properties of a polymer provides useful strength and deformation data for the plastics engineering process. It is worth noting that the properties of plastics have a high sensitivity to the rate which rate they are pulled (tension) or pushed (compression). It is important to recognize this sensitivity as properties experienced in the end application can differ from those observed during a controlled test. For this reason, ASTM D1708 and other plastics testing standards are generally used for quality control in a production setting or for comparative purposes in a R&D setting.

Materials Testing System

As typical forces will not exceed 1 kN (225 lbf) and displacements will not exceed 2 inches (50 mm), we recommend a low force single column test frame such as those found in Instron's 3400 and 6800 series.




ASTM D1708 Test Setup
1) 6800 Series Universal Testing System
2) Bluehill Universal Software
3) 2580 Series Load Cell
4) 2712-041 pneumatic side action grips

 

ASTM D1708 plastic tensile testing
Grips

Due to the low forces involved, 250 N pneumatic side action grips (2712-052) or 1 kN manual wedge grips (2716-016) should be sufficient for most ASTM D1708 testing.

250 N Model | 2712-052
2616-017
2 kN Model | 2716-017
Tips and Tricks 
  • Gripping can be a challenge when testing subsized specimens. ASTM D1708 allows a minimum specimen shoulder length (the region of the specimen that is gripped) of 8 mm, which can cause difficulties due to insufficient specimen insertion into the grip’s jaw face. When insufficient specimen insertion exists, it is recommended to use grips that do not allow jaw face pivot as it can cause unwanted stress concentrations along the specimen. With sufficient specimen insertion, Instron recommends its 250 N capacity pneumatic side-action grips (2712-052) with serrated jaw faces. With insufficient jaw face insertion, Instron’s 1 kN capacity, manual wedge action grips (2716-016) are recommended.
  • Due to their small size, microtensile specimens can increase the chances of a pinch hazard when operators clamp the specimen with pneumatic grips. Instron’s 3400 and 6800 frames have an optional Smart-Close Air Kit that is fully integrated into the frame and software. The Smart-Close Air Kit minimizes pinch hazards by closing the jaw faces at a reduced speed and pressure during installation. When the test is ready to begin full pressure is applied, and the test routine starts.
Related Content

6800 Catálogo de sistemas de ensayo Serie Premier

Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.

Serie 3400: soluciones de ensayo asequibles

Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.

Catálogo de Bluehill Universal

El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.

Mordazas neumáticas de acción lateral Serie 2712-05x

Las mordazas neumáticas de acción lateral ofrecen una solución de agarre versátil para una amplia gama de materiales. Capacidades nominales de hasta 250 N.

Mordazas de cuña manuales 2716-01x, 2716-02x y 2736-01x

La mordaza de cuña manual de Instron está diseñada para facilitar la carga, la alineación y el posicionamiento de las muestras. Tras el contacto directo inicial, la fuerza de agarre aumentará a medida que aumenta la carga de la prueba. Capacidades nominales de hasta 50 N.