ASTM D1037 Ensayo de adherencia interna de placas de fibra y adhesivos para madera
- Wood
- Tension
- ASTM D1037
ASTM D1037, the Standard Test Method for Evaluating Properties of Wood-Base Fiber and Particle Panel Materials, outlines multiple testing procedures to characterize the mechanical properties of fiberboard. The internal bond test procedure is outlined in section 11 of the ASTM D1037 standard, though other sections also evaluate fastener holding, flexure properties, and compression properties in ambient or simulated environmental conditions.
Wood fiberboard is an engineered material made by using an adhesive to glue wood chips or wood particles together under high pressure, and the internal bond test of ASTM D1037 ensures that the cohesion strength of the engineered panel is sufficient for a given application. The internal bond test measures the tensile strength of the material when applying a force perpendicular to the face. This testing is especially important considering that these materials are used in construction applications and many of them are formed through the adhesion of multiple layers of material.
Most ASTM D1037 force requirements are suitable for a dual column universal testing system such as those found in Instron's 6800 and 3400 Series. Required fixtures include Instron's 2820-061 internal bond test fixture and 2820-062 steel specimen blocks, which were designed in compliance with the requirements of this standard.
ASTM D1037 | |
---|---|
1) | 6800 Series Universal Testing System |
2) | Bluehill Universal Software |
3) | 2580 Series Load Cell |
4) | 2820-061 Internal Bond Fixture for Wood and Fiberboard |

The principle of ASTM D1037 internal bond testing involves bonding specimen blocks to the top and bottom surfaces of the test specimen with a suitable adhesive. The loading block bond must be stronger than the expected failure force of the specimen. The upper loading fixture should be self-aligning, and the specimen blocks should be 2-inch square by 1-inch in thickness and made from steel or aluminum alloy. Instron’s 2820-061 and 2820-062 fixtures have been designed in compliance with these requirements.
Related Content6800 Catálogo de sistemas de ensayo Serie Premier
Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.
Serie 3400: soluciones de ensayo asequibles
Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.
Catálogo de Bluehill Universal
El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.
Dispositivo de aplastamiento para madera 2820-061
El dispositivo de aplastamiento 2820-061 está diseñada para comprobar las propiedades de resistencia de la madera o madera laminada bajo carga de tracción.