ASTM D2256 - Standard Test Method for Tensile Properties of Yarns by the Single-Strand Method

ASTM D2256 tensile testing of yarn

ASTM D2256 is a testing standard that specifies the method for determining the tensile properties of monofilament, multifilament, and spun yarns. It provides a testing procedure for determining maximum force and elongation and provides directions for calculating other properties such as breaking tenacity and modulus. ASTM D2256 is intended to determine the quality of the raw material while aiding in quality control of the finished product.

Materials Testing System

Due to its high data capture rate, we recommend our high tier 6800 Series test frame as the optimal solution for ASTM D2256 testing, although our more affordable 3400 Series is also appropriate. A single column frame is adequate for most single-strand yarn specimens as the loads rarely exceed 5 kN. In cases where yarn specimens require greater force, a dual column system may be needed.




ASTM D2256 Test Setup
1) 6800 Series Universal Testing System
2) Bluehill Universal Software
3) 2580 Series Load Cell
4) 2714-005 Pneumatic Cord and Yarn Grips

 

ASTM D2256 system setup
Grips

The most common gripping solution for ASTM D2256 are pneumatic cord and yarn grips with smooth clamping blocks, which are well suited for testing nearly all types of yarn specimens while maintaining high throughput. A specially designed horn with a smooth finish and a contoured surface with a graduated cam allows for easy loading and a stress reduced clamping area on the specimen. By incorporating a design that evenly distributes gripping force over the surface of a curved half capstan, the chances of specimen failures are reduced. 

Instron’s 2 kN capacity cord and yarn grips can also be paired with jaw faces with several other finishes to provide adequate clamping and avoid damage to the specimens during testing. The pneumatic grips allow users to fine-tune the gripping pressure in order to avoid jaw breaks or slippage. In some cases with strong or slippery yarn specimens, use of extra padding material within the clamping blocks, such as paper or emery cloth, can also be helpful.

2714-005
1 kN Model | 2714-005
Tips and Tricks
  • ASTM D2256 is available as a pre-built test method within Bluehill Universal software. This method includes pre-configured calculations to help expedite test setup and simplify the testing process.

  • This standard recommends a Constant Rate of Extension (CRE) test frame for operating at a 20 second time-to-break, paired with grips that provide adequate clamping throughout testing. If the frame cannot provide a 20 second time-to-break or the grips allow for slippage while testing, the standard allows for alternative testing methods. These alternatives will likely be dependent on each yarn’s material properties.
Related Content

Catálogo de sistemas de ensayo Serie 6800 Premier

Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.

Mordazas neumáticas para cuerdas e hilos 2714‑005

Las mordazas neumáticas para cuerdas e hilos proporcionan un método cómodo para sujetar fibras, cuerdas, hilos y alambres finos con el fin de reducir el problema asociado con los ensayos de estos materiales. Capacidad nominal 1 kN.

Mordazas neumáticas para cuerdas e hilos 2714‑040

Las mordazas neumáticas para cuerdas e hilos proporcionan un método cómodo para sujetar fibras, cuerdas, hilos y alambres finos con el fin de reducir el problema asociado con los ensayos de estos materiales. Capacidad nominal 2 kN.

Catálogo de Bluehill Universal

El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.