ASTM D4632 - Standard Test Method for Grab Breaking Load and Elongation of Geotextiles

Written by Charlie Pryor

ASTM D4632

 

ASTM D4632 is a grab test used to determine the breaking load (grab strength) and elongation (grab elongation) of geotextile fabrics. This standard is primarily used in quality control and acceptance testing labs comparing geotextiles of similar or identical structure. It is not recommended to compare uniquely structured geotextiles or for testing knitted fabrics. It is important to review ASTM D4632/D4632M-15 in order to fully understand the test setup, procedure, and results requirements. 

 

How is the Test Performed?

The grab test is a tensile test where the central part of the specimen's width is tested to establish the "effective strength" of the fabric. The effective strength is the strength of the material at a specific width when combined with the additional strength of adjacent material. Test specimens are cut in both the machine direction and cross-machine direction, but are expected to have their results calculated separately. Specimens are cut to 101.6 mm x 203.2 mm (4 in x 8 in), with attention to the direction of the fabric.

The specimen is loaded into the grips leaving a 75 mm (3 in) separation between the jaw faces. ASTM D4632 calls for jaw faces that are at least 25.4 mm x 50.8 mm (1 in x 2 in). However, it allows for each grip to include one jaw face that is larger than the other (a modified grab test), which can be helpful in reducing the effects of specimen/jaw face alignment. The test is conducted at a speed of 300 mm/min (12 in/min) with the required results being load at break and total elongation.

Testing System

Geotextile testing requires a test system with a data rate capture high enough to measure the failure of individual fabric fibers. Because of this, Instron recommends a high tier 6800 Series test frame, which provides a data acquisition rate of up to 5 kHz and captures data peaks and valleys accurately at up to 2500 or 5000 points per second, respectively. For most geotextiles testing to ASTM D4632, a single column frame such as Instron's 68SC-5 is appropriate, as the loads rarely climb higher than 5 kN. The rapid data capture rate in Bluehill Universal software allows data peaks and valleys to be captured accurately.

ASTM D4632 test setup

ASTM D4632 Test Setup

1. Instron 68SC-5

2. Bluehill Universal Dashboard (2490-696)

3. 2580 Series Load Cell (2580-5kN)

4. 2712 Series Pneumatic Grips (2712-045)

 

 

Grips

Geotextile materials tend to have coatings that may make them difficult to test without slippage or jaw breaks. Instron’s pneumatic side acting grips provide an easy, repeatable, high throughput gripping solution that allow the user to quickly fine-tune gripping pressure to avoid jaw breaks or slippage. Pneumatic side acting grips also feature Instron’s quick-change technology which allows the jaw faces to be easily changed by hand without requiring tools or pins. Since different geotextiles can require a range of different clamping surfaces, quick-change jaw faces can significantly improve throughput in labs where these materials are common.

2712-045
5 kN Model | 2712-045

Related Content

6800 Catálogo de sistemas de ensayo Serie Premier

Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.

Catálogo de Bluehill Universal

El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.

Serie 3400: soluciones de ensayo asequibles

Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.

Mordazas neumáticas de acción lateral Serie 2712-04X

Las mordazas neumáticas de acción lateral ofrecen una solución de agarre versátil para una amplia gama de materiales. Capacidades nominales entre 1 y 10 kN.