ASTM E190, AWS B4.0 Guided Bend Test of Welds
- Metals
- Flexure
- ASTM E190
ASTM E190 describes requirements for guided bend testing of welded materials. The guided bend test on welds is designed primarily for metal plates and pipes and provides a quality control check that helps determine the ductility of the weld and the effectiveness of the welding process. During the bend test, the material containing the weld is supported on both ends by the test fixture, while a load is applied at its center point.
Materials Testing SystemFor ASTM E290 testing we recommend using an Industrial Series DX or HDX model with Bluehill Universal software and a W-6810 test fixture. This fixture allows for adjustment of the support span and is supplied with various sizes of loading mandrels to accommodate different specimen thicknesses. The loading supports are held together with two tie rods to provide extra stiffness during loading. The DX or HDX Model dual test space load frames allow the bend test fixture to be positioned in the lower compression test space. Any tensile testing can also be accomplished in the upper tensile test space.
ASTM E190 Test Setup | |
---|---|
1) | Instron 1000 HDX |
2) | W-5340 Hydraulic Wedge Grips |
3) | W-6810 test fixture |

This standard is very focused on the interpretation of the tested specimen. Bluehill Universal can easily be configured with a prompted test that allows the operator to note the condition of the tested specimen and report any cracks that are outlined by the code requirements. Digital calipers can also be interfaced directly to the software for quick, push-button input of crack measurements.
Related ContentCatálogo de máquinas de ensayo universales de alta fuerza
Los sistemas de alta fuerza de Instron incluyen sistemas de ensayo electromecánicos e hidráulicos de alta capacidad para aplicaciones de tensión y compresión. Las capacidades de fuerza van de 100 kN a 2000kN.
Modelos HDX de la Serie Industrial
Estos bastidores hidráulicos, con un espacio de ensayo doble y una pista de ensayo larga, están disponibles en capacidades de 1.000 kN (225.000 lbf) y 1.500 kN (337.500 lbf).
Catálogo de Bluehill Universal
El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.