Plastic Strain Ratio (r-value) According ISO 10113, ASTM E517, and JIS Z 2254
- Metals
- Tension
- ISO 10113
- ASTM E517
- ASTM E646
- JIS Z 2254
- JIS Z 2253
- JIS Z 2241
To calculate the r-value, a test is performed to ISO 6892 and requires the use of axial and transverse extensometers. Where the behavior of true plastic width strain versus true plastic length strain is homogeneous, a single point calculation can be used. For material that exhibits inhomogeneous deformation, a regression method is recommended, and ISO 10113:2020 strongly recommends measuring transverse strain at multiple locations evenly distributed along the axial gauge length, to be averaged into one value. The AverEdge32™ feature of Instron's AVE2 non-contacting video extensometer can provide this capability, and these calculations can be done automatically in real time using the Bluehill® Universal materials testing software.
An ISO 10113, ASTM E517, or JIS Z 2254 test is typically performed at the same time as ISO 10275, ASTM E646, or JIS Z 2253, the tensile strain hardening exponent (n-value). Sheet metal testing applications require calculations such as yield strength, yield point elongation, ultimate tensile strength, r-value and n-value. These calculations place a high physical demand on traditional contacting extensometers for measuring axial and transverse strain. They need to allow for enough travel to test the specimens through break, but small gauge lengths make it more challenging to ensure high accuracy of the measurements. Additionally, relevant ASTM and ISO testing standards have accuracy requirements that must be achieved.
Historically, video extensometry is not frequently used in these applications, as most customers in the metals industry prefer traditional contacting extensometers and trust the reliability of the results. Significant advances in the technology of video extensometry offer metals testing customers other options. Not only do video extensometers like the AVE2 allow for simultaneous collection of axial and transverse strain data and reduce the maintenance required for wear and tear on knife-edges, they have also been shown to increase productivity and simplify testing. In addition, the AverEdge32™ feature has shown substantial improvement in reducing transverse strain measurement variability.
Instron's AutoX Biaxial automatic contacting extensometer is another excellent solution for biaxial strain measurement, as it provides repeatable r-value results that are not influenced by operator input as traditional extensometers are.
AverEdge 32 de Instron
Extensómetro de vídeo sin contacto AVE 2
La segunda generación del extensómetro de vídeo avanzado (AVE 2) utiliza la tecnología de medición de deformación sin contacto más rápida y precisa disponible en el mercado.
Extensómetro de contacto automático: modelo AutoX 750
El AutoX 750 es un Extensómetro de contacto automático de alta resolución y para largas distancias. Se puede montar en cualquier sistema de mesa o modelo de suelo electromecánicos 3300, 3400, 5500, 5900 o 6800, así como en sistemas estático-hidráulicos de ensayo LX, DX, HDX y KPX. Es especialmente indicado para aplicaciones relacionadas con plásticos, metales, biomedicina, materiales compuestos, elastómeros, etc. El AutoX tiene un recorrido máximo de 750 mm y una precisión de ±1 μm.