ISO 527-3 Tensile Properties of Films and Sheets

Written by Dan Caesar

ISO 527-3 applications

plastics hub icon 

ISO 527-3 is an international standard used to determine the tensile properties of plastic film or sheeting. Plastic films are used extensively in the packaging industry and as components of more complex products, such as electric vehicle batteries. Material properties reported for this standard are tensile strength, yield point, and strain.

Film or sheeting is defined to be a plastic test specimen with a thickness less than 1 mm. Plastics with a thickness greater than 1 mm should be tested per ISO 527-2. The equivalent ASTM standard to ISO 527-3 is ASTM D882.

Separator Film Testing for Electric Vehicle Batteries

ev battery icon  

Separator films are used in EV battery production to separate the anode and cathode in lithium-ion and other liquid electrolyte batteries. These films are required in high volumes and are extremely critical to product safety. Because testing standards specific to EV batteries have not yet been established, ISO 527-3 is commonly used as a proxy standard to characterize their frictional properties. The most common material used for separator film is polyolefin, a polymer film that is strong enough to withstand the winding operation during assembly as well as uneven plating of lithium on the anode due to extensive use. Safer and stronger separator material more effectively prevents contact between the anode and cathode, while thinner material helps reduce the weight of each battery and improve energy density.


Recommended Testing Equipment

Because thin film specimens break at relatively low forces, ISO 527-3 testing is often performed on a single column universal testing machine. However, due to the fact that many thin film specimens exhibit high elongation at break, an extra height single column frame or possibly a dual column frame may be required in order to test until break. Instron's 3400 and 6800 Series include a variety of test frames suitable for thin film testing, with the 6800 Series offering many advanced features for those wishing to maximize repeatability and throughput.




ISO 527-3 Test Setup
6800 Series Universal Testing System
 Bluehill Universal Software
 2580 Series Load Cell
 Pneumatic Side-Action Grips

 

ISO 527-3 test setup
Gripping Solutions 

Due to the flexible, delicate nature of thin film specimens, specimen gripping can be a challenge. Pneumatic side action grips are an ideal solution because they provide an adjustable inlet air pressure to ensure that specimens can be clamped sufficiently throughout the test. When using pneumatic grips with the Smart-Close Air Kit, operators can define the inlet clamping pressure in the Bluehill Universal test method, replacing the need to manually change the pressure at the air supply’s regulator. The Smart-Close Air Kit not only promotes a safer use of pneumatic grips, but it can make testing more efficient and repeatable.


For those looking for a non-pneumatic solution for ISO 527-3 testing, Instron recommends self-tightening roller grips. Manually-tightened screw grips are not recommended for thin film testing, because the variability they add to the clamping pressure can negatively impact the repeatability of results and cause a higher frequency of improper gripping (jaw breaks or slippage). 

2712-041
1 kN Model | 2712-041
2613-007
1 kN Model | 2713-007

Specimen Alignment

Tensile testing of thin films and foils presents more challenges than the testing of rigid specimens. The majority of thin films and foils used in EV battery manufacturing have a thickness of no more than 15 microns, making it extremely easy to damage them during the specimen insertion process. Correctly aligning such delicate specimens is a major pain point for many testing labs, and the use of a precision specimen loader device is recommended. These devices use a detachable alignment clip and linear rail to guide the specimens into the grips, and are available in multiple sizes to accommodate a wide range of specimen dimensions.

Strain Measurement

Extensometers enable us to provide the most accurate strain measurement. Non-contacting video extensometry is the best solution for thin film testing, as typical clip-on extensometers weigh down the specimen causing premature failure. Instron's Advanced Video Extensometer (AVE2) can measure strain as accurately as a clip-on extensometer without physically contacting the specimen.

Results and Throughput

Instron's Bluehill® Universal testing software makes it easy to report calculations in compliance with the standard. Customers who choose the Plastics method suite will receive a pre-configured test method for ISO 527-3 testing, complete with specific test parameters and calculations to help ensure compliance.

For labs with high-volume testing needs, several modifications to the tensile machine setup can be made to speed up the testing process and increase throughput, up to and including fully automated test systems. Fully automated systems such as Instron's AT3 are designed to incorporate specimen measurement, specimen loading, testing, and removal, and are able to run for hours without operator interaction. These systems help to reduce variability due to human error and can be left running after a shift ends to continue getting results when operators go home.

Related Content

Catálogo de sistemas de ensayo Serie 6800 Premier

Los sistemas de ensayo universales Serie 6800 de Instron proporcionan una precisión y fiabilidad sin igual. Construida sobre una arquitectura de sistema Operator Protect pendiente de patente, con un kit Smart-Close totalmente nuevo y funciones de mitigación de colisiones, la Serie 6800 hace que los ensayos de materiales sean más sencillos, limpios y seguros que nunca.

Catálogo de Bluehill Universal

El software Bluehill Universal está diseñado desde el principio para una interacción táctil y una experiencia de usuario intuitiva. Descubre ensayos más sencillos y limpios con funciones como métodos de ensayo precargados, QuickTest en segundos, exportación de datos mejorada e Instron Connect, una nueva función que proporciona un enlace de comunicación directa con el servicio. Los usuarios de versiones anteriores del software, como Bluehill 2 y Bluehill 3, pueden actualizarse fácilmente a la última versión de Bluehill.

Precision Specimen Loader

The Precision Specimen Loader for Thin Films provides a safer, more ergonomic, accurate, and more convenient way to load thin film and foil specimens into Instron 2712-052 grips.

Serie 3400: soluciones de ensayo asequibles

Sistemas de ensayo universales Serie 3400 de Instron para ensayos de tracción, compresión, doblado y otros materiales.

Mordazas neumáticas de acción lateral Serie 2712‑04X

Las mordazas neumáticas de acción lateral ofrecen una solución de agarre versátil para una amplia gama de materiales. Capacidades nominales entre 1 y 10 kN.

Mordazas de rodillo autontensora Serie 2713‑007

Las mordazas autotensoras están diseñadas principalmente para la realización de ensayos de precisión de materiales elastoméricos y otros materiales flexibles que presentan una gran reducción del área de la sección transversal bajo carga.

Extensómetro de vídeo sin contacto AVE 2

La segunda generación del extensómetro de vídeo avanzado (AVE 2) utiliza la tecnología de medición de deformación sin contacto más rápida y precisa disponible en el mercado.